I'm looking for a new wheel head, for one of my classroom wheels.  It is an Amaco Number 1.  I've looked in a dozen places, and the only thing I've really been able to find, is the recessed wheel heads, which is what I currently have and really dislike. 

 

I looked on some of the auction and surplus sites, but no luck yet.

Share this post


Link to post
Share on other sites

have you contacted amaco?  You might be able to find a suitable replacement if you tell us how the current one connects to the wheelhead (recessed fitting with a set screw, etc) as well as the dimensions of those attachment points.

Share this post


Link to post
Share on other sites
Benzine    610

So after dragging my feet, and searching in many different places with no luck, I finally contacted Amaco.  They do make a flat wheel head, for the wheel, but they are out of those, for my axle size, and are not currently producing them. 

They will contact me, once they restart production, but have no idea when that is.

 

I guess I'll keep looking. 

 

In the mean time, if anyone comes across a flat wheel head for a Amaco Number 1 wheel, that fits a 5/8" axle, give me a holler. 

Share this post


Link to post
Share on other sites
Mark C.    1,807

How about having another brand head drilled out by a machine shop to your shaft size?

Mark

Share this post


Link to post
Share on other sites
Pres    896

Mark's solution seems good to me. At the same time if your district has a vo tech as most do after dropping shop classes, I would check with them. They may be able to manufacture something for you, or make recommendations on what to purchase that they could modify as Mark says. If you fiind one with too large a hole a collet insert could be made.

Share this post


Link to post
Share on other sites
Benzine    610

Sounds like a good possible solution.

Are there wheel heads with a bore smaller than 5/8"? I haven't come across any.

Share this post


Link to post
Share on other sites
Mark C.    1,807

A machine shop can put in an insert and drill that out to whatever you need-most wheel heads are aluminum which work well with inserts.

Mark

Share this post


Link to post
Share on other sites
Benzine    610

A machine shop can put in an insert and drill that out to whatever you need-most wheel heads are aluminum which work well with inserts.

Mark

Ah, got ya. I'll check with my Industrial Tech Department, yes Pres we are lucky enough to still have one, and seen what they can do. Otherwise, there is a machine shop a block from my house.

Share this post


Link to post
Share on other sites
Mark C.    1,807

An all aluminum head can gave have heli coil installed in shft hole then drill out whatever hole size is needed-The drill has to be a perfect 90 degrees  to head plane.

Any machine shop can do this-

I will go measure my brent wheel head banding wheel made from old head for shaft size diameters-back with that soon-need to mix some glazes today anyway.

Mark

 

I measured my old Brent 14 inch  (from the 70s) wheel head converted to a Banding wheel.

The old Brent shaft is 5/8th exactly what you are looking for.I have not measures a newer Brent shaft-they may be bigger-I recall that that may be the case.

How about calling Amaco/Brent and talking to the Brent technical about a 5/8 wheel head

The brents are held in with a roll pin ponded in and never removed except drilling them out as they are at an angle

You could drill a new hole at a 90  in the head and get a roll pin from brent as well for the new head you order?

Options many options.

Mark

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×