      Ceramic Arts Network is looking for two new forum moderators for the Clay and Glaze Chemistry and Equipment Use and Repair sections of the Ceramic Arts Network Community Forum. We are looking for somebody who is an active participant (i.e. somebody who participates on a daily basis, or near daily) on the forum. Moderators must be willing to monitor the forum on a daily basis to remove spam, make sure members are adhering to the Forum Terms of Use, and make sure posts are in the appropriate categories. In addition to moderating their primary sections, Moderators must work as a team with other moderators to monitor the areas of the forum that do not have dedicated moderators (Educational Approaches and Resources, Aesthetic Approaches and Philosophy, etc.). Moderators must have a solid understanding of the area of the forum they are going to moderate (i.e. the Clay and Glaze Chemistry moderator must be somebody who mixes, tests, and has a decent understanding of materials). Moderators must be diplomatic communicators, be receptive to others’ ideas, and be able to see things from multiple perspectives. This is a volunteer position that comes with an honorary annual ICAN Gold membership. If you are interested, please send an email outlining your experience and qualifications to jharnetty@ceramics.org.
Sign in to follow this  
Pnutbrand

Making A Kiln Lid

Recommended Posts

I was wondering if anyone has any suggestions on the type of cement to use to make a new kiln lid. Have been searching but haven't found anything that's made for lids, most cements I have found say not to use on lids. I am in the process of making a new gas kiln and would like to cement this one instead of drilling and cinching with all thread as I did on the last kiln. I have some amaco kiln cement, would this work? Will be firing mostly to cone 5-6 with an occasional cone 10.

Share this post


Link to post
Share on other sites

I think that any kiln lid you construct will have to have some form of compression support at the circumference. Over the years I do not recall ever seeing in books or studios a lid without some form of external support-angle iron and threaded bars etc. I would check the library on kiln construction if you haven't already.

Share this post


Link to post
Share on other sites

Is this a typical front loading gas kiln? If so, just build an arch. It's just as quick and infinitely stronger. I wouldn't trust mortar to hold together the top of a kiln that is any more than 28 inches across. Give us some more info about the kiln. Size, shape, wall thickness, materials, etc.

Share this post


Link to post
Share on other sites

Is this a typical front loading gas kiln? If so, just build an arch. It's just as quick and infinitely stronger. I wouldn't trust mortar to hold together the top of a kiln that is any more than 28 inches across. Give us some more info about the kiln. Size, shape, wall thickness, materials, etc.

Arches are elegant and very strong. We use that design on larger kilns. Should you decide to make a flat top, here is a video that shows how to cement the bricks together. As you will see, making a lid is an art form. The people who cement lids for a living are as skilled as brick layers. Note that the bricks are not sprayed with water, because the cement is applied very rapidly to the bricks. The long pan is essential.

 

 

 

Sincerely,

 

Arnold Howard

Paragon Industries, L.P., Mesquite, Texas USA

ahoward@paragonweb.com / www.paragonweb.com

ruddhess and ivolucien like this

Share this post


Link to post
Share on other sites

Thanks for the replies. The kiln is going to be top loading square kiln, 36" square outside with 4.5" wall thickness giving it 27" square inside. Using 9x3x4.5" 2600 IFB with a hard brick around the gas ports to prevent damaging soft bricks. It will have 2 intake ports and a downdraft exhaust. Will be using propane as a fuel source. And yes I reckon I do mean mortar instead of cement. Was also considering making it a two piece lid for weight purposes. Ill be lifting on and off most likely unless I decide to fabricate a hinge system.

Share this post


Link to post
Share on other sites

Not sure where you live but the right cement can be had from Hi-Temp in Portland Or, it comes in 5 gallon buckets and can be shipped-they make it themselves on site-I have used the super 33 for gluing bricks but they have another made for skutt kilns that would be a better choice.Call them and talk to them-they are not a potters supply  business but will sell you a tub.Ask for Jeff

Mark

Share this post


Link to post
Share on other sites

I would also look at adding a layer of fiber board to the outside of the kiln to increase the insulation value and tightness.

I considered that. At the moment it has a sheet metal covering inside a welded angle iron frame.

Share this post


Link to post
Share on other sites

I need to build a new kiln lid, flat type with sheet metal round the outside bolted into tension. This is more a reminder to myself to watch the video as I can't seem to watch it at work.

 

Just one question, kiln cement/mortar doesn't need firing for it to work? Anybody in the UK know of a good make/type?

Share this post


Link to post
Share on other sites

 

Just one question, kiln cement/mortar doesn't need firing for it to work? Anybody in the UK know of a good make/type?

. Suggest you buy from a kiln builder - Pottery crafts? Potclays, ......

Share this post


Link to post
Share on other sites

Does the lid have to be brick? My homemade gas kiln is top loading. The lid is a frame of stainless steel with a couple of bits of angle aluminium across the top from which homemade ceramic buttons on shanks of kanthal element wire, suspend 5 inches of ceramic fibre. I get into the kiln by lifting each side onto a hook and swing it out of the way.

Share this post


Link to post
Share on other sites

Fiber blanket is best used in applications where it is not moved. Each time fiber blanket is moved or touched it releases fibers into the air which can be inhaled. Inhaling fiber is not good for your lungs. Yes, it is light weight and insulates well, but it is by no means durable and is the least safe kiln building material to work with.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.