I have a old electric kiln that is only 2" thick and I have already purchased a gas conversion kit. It is an updraft kiln design. I would like to do reduction firing in it with slow cool downs. Can I put ceramic fiber on the outside of the kiln and then dry stack hard brick around the outside to insulate it? Would that be enough for slow cooling? I have about 900 hard brick from an old beehive kiln that I'm trying to find a use for...

Share this post


Link to post
Share on other sites

jack up the kiln w/ bricks. cause you'll need to build a chemney.

what ^ was the kiln rated for?

as long as your the only one using it - definetly wrap w/ fiber blanket-

I've found that students are hard on it

Sounds like your going to have some fun!

Firing to ^ 6r?

 

 

Share this post


Link to post
Share on other sites

jack up the kiln w/ bricks. cause you'll need to build a chemney.

what ^ was the kiln rated for?

as long as your the only one using it - definetly wrap w/ fiber blanket-

I've found that students are hard on it

Sounds like your going to have some fun!

Firing to ^ 6r?

 

 

 

I'll be firing to Cone 10, I used to fire to cone 6 in it but it was rated for cone 10. I plan to use natural gas. It has an extra ring on it that I thought about making a pully for so I could use it for Raku some of the time. It will be exclusively used by me but I've never fired a gas kiln myself so I am a little timid about it. If it is a 3 1/2 cubic foot kiln how tall should the chimney be?

Share this post


Link to post
Share on other sites
Guest JBaymore

Nope... no chimney for an updraft needed. However a short small "extension" from the exit flue port in the lid made of (light) IFB will help to even out the temperature at the very top of the chamber rather than just having a "hole in the lid". Doesn't have to be long..... 9" high is plenty. Same size XC as the hole in the top. I'd also recommend a half shelf located directly under the flue opening and above the top of the last shelf of work........ making sure that the space between that shelf and the bottom interior surface of the lid is adequate to match the XC of the flue opening in square inches of flow area.

 

And if you wrap fiber around the outside of the kiln without removing the metal jacket, you will bring the interface temperature of the point where the fiber is against the metal and the inner firebick layer up to a point that will quickly destroy the metal jacket. It was never designed to get that hot. Even if it is stainless. It will quickly rust out. The more you insulate it, the worse the problem. BUT.... if you remove the metal jacket on the firebrick that acts as the "tensioner" that compresses the insulating firebrick into istelf, the kiln structure will sort of "fall apart.

 

So insulating the exterior is not quite as simple as "wrapping" the kiln like you might a hot water heater in a house with pink fiberglass.

 

Insulating the floor and lit on the outside however is a snap.

 

And it you are working with RCF (fiber).... PLEASE check out the MSDS for that stuff to know well what you are working with BEFORE using it. And check out the European Union standards fior RCF online. An eye opener.

 

 

best,

 

......................john

Share this post


Link to post
Share on other sites

Nope... no chimney for an updraft needed. However a short small "extension" from the exit flue port in the lid made of (light) IFB will help to even out the temperature at the very top of the chamber rather than just having a "hole in the lid". Doesn't have to be long..... 9" high is plenty. Same size XC as the hole in the top. I'd also recommend a half shelf located directly under the flue opening and above the top of the last shelf of work........ making sure that the space between that shelf and the bottom interior surface of the lid is adequate to match the XC of the flue opening in square inches of flow area.

 

And if you wrap fiber around the outside of the kiln without removing the metal jacket, you will bring the interface temperature of the point where the fiber is against the metal and the inner firebick layer up to a point that will quickly destroy the metal jacket. It was never designed to get that hot. Even if it is stainless. It will quickly rust out. The more you insulate it, the worse the problem. BUT.... if you remove the metal jacket on the firebrick that acts as the "tensioner" that compresses the insulating firebrick into istelf, the kiln structure will sort of "fall apart.

 

So insulating the exterior is not quite as simple as "wrapping" the kiln like you might a hot water heater in a house with pink fiberglass.

 

Insulating the floor and lit on the outside however is a snap.

 

And it you are working with RCF (fiber).... PLEASE check out the MSDS for that stuff to know well what you are working with BEFORE using it. And check out the European Union standards fior RCF online. An eye opener.

 

 

best,

 

......................john

 

 

Thank you for the response :). Now that you mention it I do remember reading archives on Clayart from others who have converted an electric kiln saying that the kiln won't last long. That must be why. I will check out the European Union standards before using the RCF, thank you. So should I not worry about the exterior of the kiln, just insulate the tope and the bottom?

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.