Posted 12 September 2013 - 08:46 PM

I had a relay fail during a Cone 5 glaze firing. The temp reached 1800 degrees and fired 10 and a half hours. The glazes were under fired  and looked chalky but they do not come off. I have replaced the bad relay and my question is: do I re-glaze before re-firing, just re-fire, or do I just throw the stuff away? 



#2 oldlady

oldlady

    single firing an electric kiln to cone 6

  • Members
  • PipPipPip
  • 3,447 posts
  • Locationharpers ferry west va and pinellas park fl

Posted 12 September 2013 - 09:27 PM

if your kiln is current, not an extra old one, contact the manufacturer.  they have someone who will help you with this.


"putting you down does not raise me up."

#3 Min

Min

    Advanced Member

  • Members
  • PipPipPip
  • 1,520 posts
  • LocationCanada

Posted 12 September 2013 - 09:43 PM

Refire to ^5, the glazes will be fine. If you got to 1800F that is only ^06 so your glazes haven't melted yet, therefore the chalky appearance.



#4 bciskepottery

bciskepottery

    Advanced Member

  • Moderators
  • 2,703 posts
  • LocationNorthern Virginia

Posted 12 September 2013 - 09:43 PM

You should be able to refire the glaze load.  The glaze is probably underfired; so, taking it up to the correct temperature should allow it to melt correctly. 



#5 sivamc

sivamc

    Newbie

  • Members
  • Pip
  • 3 posts

Posted 12 September 2013 - 10:04 PM

Thank you all.  I thought that I could just re-fire.



#6 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 5,045 posts
  • LocationGrayslake, IL

Posted 13 September 2013 - 08:36 AM

If your relays have not been replaced in a few years, go ahead and replace them all. Chances are the others will fail soon, too. Write the date on the new ones with a marker so you'll know how old they are next time they fail.


Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

neil@neilestrickgallery.com






0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users