Hi,

 

Thanks for the replays to my question about what temp to fire pclay over metal. I fired a some pieces at 04 and one at 06. O4 pieces seemed to be more fragile. Now...can these pclay over metal be refired? If so, again to what temp.

 

I really like the forum. I think it would be great to have one just for paper clay.

 

Thanks

Share this post


Link to post
Share on other sites

Yes, you can fire them again ...

The limits on the temp would be decided by the melting point of your metal and the cone your clay fires to.

 

 

Thanks Chris,

 

I appreciate that you are so willing to help and so prompt in your responses.

 

Thanks again.

 

Acg

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.