You can spray a dipping, pouring or brushing glaze. If it is a commercial brushing glaze it probably has gums and flocculants added to it to make it thick. If this is the case then you can either water it down just enough so it sprays or you can use a deflocculant (sodium silicate or Darvan). Increasing the psi of the compressor also helps spray a thick glaze, I spray one of my glazes on when it is a yogurt consistency this way.