Slips And Engobes?

Recommended Posts

oldlady    1,323

simple answer.  slip is very wet clay.  it will stick to clay.  wet or damp clay.  not fired clay.  do not try to put it on fired clay.  it will flake off.

 

 

engobes are coverings for clay that contain several ingredients and may be used after clay is fired.  this is not the only answer but might help.

 

i am sure someone will criticize this answer.  it is simple because the question is simple.  i do not believe in making things complicated.