I bought engobes powder.

Can anyone tell me if when I put water in engobe powder, I add with the water some substance to stick with engobe glazed effects?  :blink:

Share this post


Link to post
Share on other sites
elcimen    2

It depends on what substance you are talking about. colorants?

 

Marcia

Speak of glycerin, olive oil ....
Adding a bit in for horizontal sliding engobe colors do not mix?

Share this post


Link to post
Share on other sites
elcimen    2
Bought a covering premixed dry.

Can anyone tell me if when I put water in engobe powder, I add with the water some substance to stick with engobe glazed effects?   glycerin, olive oil .... ?

I'll slide the engobe in various colors using the Slip Trailers.

I want the colors do not mix.

Share this post


Link to post
Share on other sites
bciskepottery    925

The commercial engobes I bought just required adding water, then mixing. Did not need to add anything else. Adding glycerin, olive oil, or baby oil will make them easier to apply with a brush, but they will also take a bit longer to dry.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×