Coating Soft Bricks For Soda Kiln

Recommended Posts

Kristin_Gail    12

I'm finally set on what I'm using to coat the soft bricks in my electric-to-soda kiln conversion project.   Now I wonder:  Do I have to cook it on before I fire it with pieces inside?  

 

I've read that I need to bring it to bisque temp, empty - if so, why?  Is there a reason I can't just paint it on today, load it tomorrow with pieces,fire it (now full) the next day?  I single-fire, super-slow for the first few hours, if that makes a difference.

Share this post


Link to post
Share on other sites
TJR    359

I agree. It depends on the coating. If it is alumina hydrate, and it falls on yor glazed ware,you will have white crudon the worst possible spor-like the rim of a teacup.

You could always bisque your pots with the coating.-Ha Ha-I kid!

TJR.

Share this post


Link to post
Share on other sites
TJR    359

So the reason to cook it on first is just in case it's going to fall off that very first time?

Yes. Alumina is very refractory. In other words, it melts at a high temperature. If it falls onto your glazed pots, you will have white crud.

TJR.

p.s. It was a good mix to apply. Basically kiln wash. Good luck with the firing.

T.

Share this post


Link to post
Share on other sites
Mark C.    1,798

I would run a bisque 1st in that kiln so its shrunk some before the glaze temp shrinks it more-that way you will also see how its adhering.

I always bisque coatings on but thats me-You could also deck the whole load over with a top shelve to keep the stuff from dropping-we do that in our salt kiln always as well.

That EPK will shrink a lot as its not calcined (bisqued 1st) you want it to hold the alumina which has zero sticking power.

Mark

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×