Ugh I messed up. Very early this morning I set my kiln up for a glaze fire. I think in my sleepy stupor I accidentally set my kiln sitter up with a 06 cone not cone 6. The reason I think this is because it normally takes 8 to ten hours for my kiln sitter to flick off but when I went to check on it at about 6 hours it was off. I was very confused at first but i am now rethinking my steps and realized what I've done. I can not for the life of me see the cones I set up to monitor so that won't help me

What would you more experienced potters recommend I do. Leave it to cool and then set it up again tomorrow or manually reset and put it on high for the last 2 to four hours?

Thanks in advance for your guidance.

#2 OffCenter

OffCenter

    Advanced Member

  • Members
  • PipPipPip
  • 1,372 posts

Posted 18 July 2013 - 06:29 PM

Ugh I messed up. Very early this morning I set my kiln up for a glaze fire. I think in my sleepy stupor I accidentally set my kiln sitter up with a 06 cone not cone 6. The reason I think this is because it normally takes 8 to ten hours for my kiln sitter to flick off but when I went to check on it at about 6 hours it was off. I was very confused at first but i am now rethinking my steps and realized what I've done. I can not for the life of me see the cones I set up to monitor so that won't help me

What would you more experienced potters recommend I do. Leave it to cool and then set it up again tomorrow or manually reset and put it on high for the last 2 to four hours?

Thanks in advance for your guidance.

 

I don't understand how you can manually reset the kiln sitter without letting it cool so that you can put a cone 6 in it.

 

Jim


E pur si muove.

"But it does move," said Galileo under his breath.

#3 Jo-Ann

Jo-Ann

    Advanced Member

  • Members
  • PipPipPip
  • 60 posts
  • LocationOntario, Canada

Posted 18 July 2013 - 06:37 PM

When I push the button down it stays down. Even if the latch isn't up. . . Now you have me wondering, Is that not supposed to happen?

#4 Jo-Ann

Jo-Ann

    Advanced Member

  • Members
  • PipPipPip
  • 60 posts
  • LocationOntario, Canada

Posted 18 July 2013 - 06:42 PM

Oh and I wouldn't put a cone in it I would just go by time . . .

#5 Jo-Ann

Jo-Ann

    Advanced Member

  • Members
  • PipPipPip
  • 60 posts
  • LocationOntario, Canada

Posted 18 July 2013 - 07:13 PM

I think too much time has passed so my timing would be off . . . ill just retry after it cools thanks anyway.

#6 Min

Min

    Advanced Member

  • Members
  • PipPipPip
  • 1,562 posts
  • LocationCanada

Posted 18 July 2013 - 07:20 PM

If you had the correct witness cones in the kiln I would keep the same ones in for the next firing to ^6, they have already had some heatwork like the pots have. If not I wouldn't worry about it, just put a ^6 or ^7 (which ever you usually use) in your sitter and start again. The heatwork effect of a ^06 on ^6 clay isn't going to be much. I wouldn't have gone just by time fired in the first place. 

Min



#7 Jo-Ann

Jo-Ann

    Advanced Member

  • Members
  • PipPipPip
  • 60 posts
  • LocationOntario, Canada

Posted 18 July 2013 - 07:37 PM

Thank you Min, that info helps a lot.

#8 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,463 posts
  • LocationRed Lodge, Montana

Posted 18 July 2013 - 08:28 PM

I can restart mine just by pushing the button even with the cone down. Just let it cool. Open it up and see what happened.

Marcia


Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#9 Jo-Ann

Jo-Ann

    Advanced Member

  • Members
  • PipPipPip
  • 60 posts
  • LocationOntario, Canada

Posted 19 July 2013 - 10:28 AM

Thanks Marcia,

Everything was as fine as Min said it would be. I've restarted, this time with the proper cone in the sitter. :/