Let's say I'm making a colander or a strainer, such as a berry bowl...I have a hole cutter, which works, but are there any neat tips that anyone can share to make a pattern? Or for cleaning the cut holes?

Share this post


Link to post
Share on other sites

Have you tried using a pie lattice roller on a slab of paper clay.  The clay can be stretched over a hump mold.  The cuts in the clay from the lattice roller open up into a small diamond pattern, just like on the top of a cherry pie.

 

Many use a star like pattern of holes, kind of like chinese checkers on the bottom of their thrown bowls. This still means a lot of individual holes.

 

Have fun.  Jed

Share this post


Link to post
Share on other sites

You can buy special clay cutters in shapes with plungers, the ones I have are by Kemper. I have the round, square, oval, teardrop, and star shapes. They have a few more as well like triangles and lilacs that I don't have. They work really well and I use them for miniature lanterns.

 

Terry

Share this post


Link to post
Share on other sites

Countersink drill bit for rounding the sharp edges of round holes. Straws work well for punching holes, the clay usually stays in the straw so you just snip of the end and punch through the next hole.   Min

Share this post


Link to post
Share on other sites

Back when I made colanders I tap centered them and scored some rings as the pot spun slowly. Then I used a cordless drill bit -about 1/4 inch so glaze would not fill the holes. If you pick the time right in terms of dryness then smoothing the holes will not be needed.I drilled them in a every other ring pattern by eyeball. You will get good at this after 10-20 of them.

mark

Share this post


Link to post
Share on other sites

Mostly I'm putting 1/8 inch holes in buttons, rather than larger holes, but I like to use a plastic drinking straw type coffee stirrer when the clay is leather hard.  Just back it up with a finger (or the ware board with buttons) and press the straw through, it usually leaves a nice clean hole.  I normally clear the straw out (squash it and force the clay out, or just cut the plugged up end off) after about an inch of stuff packs in there because the cuts get sloppy if the clay doesn't slide up into the straw. A minimal amount of cleaning is all thats needed this way.  I've done bigger holes with a standard straw too, seems to work just as well scaled up!  Although with something like a strainer a good drill bit might work better!

Share this post


Link to post
Share on other sites

To give your holes a beveled edge with ease, take your basic double sided loop tool (the round end) and rotate it inside of the hole.  Becuase the loop tool is bigger, it will bevel just the top of the hole, leaving a 45 degree trimmed edge. Its best to do this step at an advanced leather hard state. Good luck!

Share this post


Link to post
Share on other sites

I have used a lot of different cutters, both purchased and handmade with local material. When I taught HS I bought brass pipe in the hobby stores. You can find this item in different profiles, and lengths of about a foot. I used square or rectangle ones for individual window panes, round ones for teapot strainers, and oval ones for decoration. Cut them with a hack saw at least a 45 degree angle or more., then remove the burr with a sharp knife(wear gloves). Push iinto cheese to leather hard clay carefully, remove the plug from the pipe with a smaller piece of pipe. Out of one pipe you can get at least 3 tools. I also like a curved knife that is very sharp and has a wide tang. These are by Van Gilder, and you turn the knife as you go in getting the hole the size you want.  For tapering the edge and clean up of round holes,  I use wooden dowels of different diameters sharpened in a pencil sharpener. These smooth and compress the rim of the hole. Square holes I just rub over inside with a scungy pad when leather hard.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.