Hi, our mid fire bisque firing accidentally fired to cone 6. Needless to say the owner feels terrible. So we all want to know if there are any tips for glazing at this point or if it's futile. Any suggestions would be greatly appreciated! There's alot of sad people down there.

Share this post


Link to post
Share on other sites
Chris Campbell    1,088

No need to panic ... This has happened often.

 

The glazes will have a hard time sticking to the surfaces. One idea is to warm the pots in a low ... 200 degree F oven ... then glaze them. Glaze will adhere and everyone is happy.

You can also add gums or CMC ... But warming them in an oven is quick and easy

Share this post


Link to post
Share on other sites
katzcamp    0

No need to panic ... This has happened often.

 

The glazes will have a hard time sticking to the surfaces. One idea is to warm the pots in a low ... 200 degree F oven ... then glaze them. Glaze will adhere and everyone is happy.

You can also add gums or CMC ... But warming them in an oven is quick and easy

 

 

Chris, somebody down here was asking if a microwave would work? No oven on site.

Share this post


Link to post
Share on other sites
Pres    896

No oven, use a kiln! or even a heat gun. All you are looking for is a bit of heat to make the glaze liquid evaporate faster.

Share this post


Link to post
Share on other sites
cracked pot    7

No need to panic ... This has happened often.

 

The glazes will have a hard time sticking to the surfaces. One idea is to warm the pots in a low ... 200 degree F oven ... then glaze them. Glaze will adhere and everyone is happy.

You can also add gums or CMC ... But warming them in an oven is quick and easy

 

 

Chris, somebody down here was asking if a microwave would work? No oven on site.

 

 

I've used the microwave to heat pots I want to refire. It helps the glaze to stick to already glazed surface. Maybe it would work for you on unglazed pots as well.

Share this post


Link to post
Share on other sites
Marcia Selsor    1,301

If your glaze has high clay content , it will stick.

To glaze over fired bisque, as everyone has mentioned, heat the pot. Heat guns work well.

If the glaze is thin, heat again and dip. Keep adding until you get the enough on the pot.

 

Marcia

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×