Iforgot Posted June 28, 2013 Report Share Posted June 28, 2013 Hey Potters, I need a grey or lavender celadon glaze for cone 6 oxidation that is compatible with a white stoneware body rather than a porcelain. Thank you so much! Darrel Link to comment Share on other sites More sharing options...
OffCenter Posted June 28, 2013 Report Share Posted June 28, 2013 Hey Potters, I need a grey or lavender celadon glaze for cone 6 oxidation that is compatible with a white stoneware body rather than a porcelain. Thank you so much! Darrel Probably the easiest way to get a lavender fake celadon is by adding very small amounts of Mason stain to a clear glaze. Jim Link to comment Share on other sites More sharing options...