I want to put terra sig on greenware, bisque, then brush on and wipe off oxides or even black Lug underglaze to highlight texture. The one time I tried this, the oxide sat on top of the bisqued terra sig but would not soak in or even really attach to the pot. Suggestions, please?

Share this post


Link to post
Share on other sites
Marcia Selsor    1,301

Sounds like your terra sig sealed. Maybe try bisque firing to a lower temp. But then you may not get the desired look of the terra sig.

 

Marcia

Share this post


Link to post
Share on other sites
Chris Campbell    1,088

You are fighting the nature of terra sig which is to give you a beautiful smooth sealed surface. A good terra sig leaves no little holes for your underglaze to grab onto which is why it doesn't. You will have to get your look a different way.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×