I can't visualize the type of chuck needed to turn a foot on a bowl, platter, with an altered rim. It will need to be a wet chuck because my piece will be ready
to trim in a couple of days. Would it be a large mound of clay roughly the size of the base for support and high enough so the rim doesnt touch the wheel head?
Any and all information would be helpful. "I'm trying to think, but nothings happening".
juli

La Paloma Texas Pottery, Juli Long


#2 Benzine

Benzine

    Socratic Potter

  • Members
  • PipPipPip
  • 2,412 posts
  • LocationThe Hawkeye State

Posted 17 June 2013 - 10:59 AM

A picture, or at least description of the rim would help.

But, a mound of centered clay, as you described, should work. Put a couple scrap pieces of cloth on the centered mound, so the platter doesn't stick.
"Anything worth believing, is worth questioning"

#3 JLowes

JLowes

    Clay Doodler

  • Members
  • PipPipPip
  • 266 posts
  • LocationAtlanta Georgia area

Posted 17 June 2013 - 01:55 PM

As Benzine suggests, making a large clay chuck is one way to make the support for trimming a platter. I like the idea of cloth to keep the platter from sticking, but I also use plastic wrap over the chuck to keep the trim item from sticking to the chuck. I like this, as it keeps the clay in the chuck ready to be wedged and used again.

Another method is to use thick foam, or layers of foam built up, to support the platter while trimming. I have a bat I made using foam that I use to trim. If the rim is wider than my foam bat, I use that, and build up foam support as needed. Keep the wheel speed low, and carefully work the platter on center to trim. Cautions are catching the trimming tool on too soft clay and gouging or jerking the piece off center. I frequently trim too soft and learned the cautions the hard way.

John

#4 Mark C.

Mark C.

    Advanced Member

  • Members
  • PipPipPip
  • 6,129 posts
  • LocationNear Arcata Ca-redwood rain forest

Posted 17 June 2013 - 02:39 PM

I use a large bat with foam glued to it-works for many forms.
Mark
Mark Cortright
www.liscomhillpottery.com

#5 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,207 posts
  • LocationRed Lodge, Montana

Posted 17 June 2013 - 03:50 PM

I have a bat with 2" foam as mark describes. If this won't work for your altered rim, try putting a 1-2" thick clay coil on the rim of a coffee can. Center the can and attach with clay.
you can lay a thin piece of oam on top of that. I have added some water to the can to help give it some weight if needed. It really depends on how altered a shape you have to work with.

Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#6 Juli Long

Juli Long

    La Paloma Texas Pottery

  • Members
  • PipPipPip
  • 124 posts
  • Locationtexas

Posted 17 June 2013 - 04:31 PM

Thanks for all the good suggestions. All are workable for me. I just got stuck with thinking a chuck was the only way and forgot all the standard ways to trim. Must be the 98 degree day, with humidity!
juli

La Paloma Texas Pottery, Juli Long


#7 MichaelP

MichaelP

    Advanced Member

  • Members
  • PipPipPip
  • 190 posts
  • LocationIL/WI border

Posted 17 June 2013 - 07:35 PM

Must be the 98 degree day, with humidity!

..or, maybe, the answer is in your screen name... :D

#8 Juli Long

Juli Long

    La Paloma Texas Pottery

  • Members
  • PipPipPip
  • 124 posts
  • Locationtexas

Posted 17 June 2013 - 09:10 PM

Too funny! It is a great screen name if I may say so myself!
J

La Paloma Texas Pottery, Juli Long


#9 MichaelP

MichaelP

    Advanced Member

  • Members
  • PipPipPip
  • 190 posts
  • LocationIL/WI border

Posted 18 June 2013 - 01:09 AM

True.




0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users