I'm hoping someone knows of a commercial version or a recipe for a darker grey (not brown or buff) groggy throwing clay-body. Ideally cone 6 but cone 10 would work too. Any help would be much appreciated.
Thanks in advance,
Paul

#2 trina

trina

    Advanced Member

  • Members
  • PipPipPip
  • 437 posts

Posted 13 June 2013 - 12:55 PM

are you up to wedging colourant into a white body?

#3 oldlady

oldlady

    single firing an electric kiln to cone 6

  • Members
  • PipPipPip
  • 1,649 posts
  • Locationharpers ferry west va and pinellas park fl

Posted 13 June 2013 - 09:15 PM

i assume you have checked all the clay suppliers online catalogs for grey or black clays. if you haven't, start there.
"putting you down does not raise me up."

#4 RPMpottery

RPMpottery

    Member

  • Members
  • PipPip
  • 12 posts

Posted 14 June 2013 - 06:49 PM

i assume you have checked all the clay suppliers online catalogs for grey or black clays. if you haven't, start there.



I've checked all that I know of. Looks like using stains is the way to go.

#5 Biglou13

Biglou13

    Advanced Member

  • Members
  • PipPipPip
  • 1,172 posts
  • LocationNorth Florida

Posted 14 June 2013 - 07:00 PM

Wedge together a black clay body and a white one?


http://claystore.alf...04 Cookbook.pdf

Some black clay bodies there
Caution big brother is watching.
The beige is blinding!!!!!!
The middle of the road is boring

The true sign of intelligence is not knowledge but imagination.
-Albert Einstein




0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users