Posted 10 June 2013 - 02:06 PM

is there a way to keep from pushing the leather-hard pot out of round while carving the sgraffito pattern? does anyone slightly fire the pot before carving, or does that make the carving too difficult?
thanks.

#2 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,117 posts
  • LocationRaleigh, NC

Posted 10 June 2013 - 04:48 PM

This is one area where you just have to wait until the pot has set up a bit ... I call it cheese hard ... like cheddar cheese for me. Some people like to carve earlier or later, depends on what tool you are carving with and how sharp it is. You can't really carve much into soft clay without distorting it but some people like that effect too.
Chris Campbell Pottery
Contemporary Fine Colored Porcelain
http://ccpottery.com/

>TRY ... FAIL ... LEARN ... REPEAT"

" If a sufficient number of people are different, no one has to be normal "

Fredrick Bachman

#3 Pres

Pres

    Retired Art Teacher

  • Moderators
  • 3,179 posts
  • LocationCentral, PA

Posted 10 June 2013 - 05:16 PM

As Chris says, cheese hard is the earliest time to do sgarffito unless you want to deform the pot. I also work on leather hard after a slip coating to give me a little crisper edge. I use a notched squidgy to push and pull slip in a form like sgraffito but in the end cheese to leather hard
Simply retired teacher, not dead, living the dream. on and on and. . . . on. . . . http://picworkspottery.blogspot.com/

#4 annekat

annekat

    Advanced Member

  • Members
  • PipPipPip
  • 44 posts
  • LocationOlympia, Washington

Posted 10 June 2013 - 05:57 PM

I also find that I have better control over the line that the tool makes if the clay is a little harder and doesn't gouge in as much while incising.... however, too dry, and the tool will start slipping around and you will lose control again. Also, when painting slip on the pot, it may make the clay a little softer than it was. If the clay is on the dry side of "cheese hard", it may suck up some of the moisture from the slip and be just right. There are so many variables, such as the thickness of the clay, how much slip you are applying, etc. It's all trial and error within your personal working methods. But if you are getting deforming, starting with a somewhat drier pot should help.
Anne

#5 Kohaku

Kohaku

    Huffing cobalt over a Raku kiln

  • Members
  • PipPipPip
  • 331 posts
  • LocationMoscow, Idaho

Posted 10 June 2013 - 07:55 PM

I tend to incise deeper lines than is typical for sgraffito, and there's definitely a 'sweet spot'. I like things a little harder than is typically referred to as 'cheese hard'- hard enough to yield sharp, clean, flowing lines without the tool catching or any fracturing in the clay.

It's a surprisingly finite range... but glorious when you find it.
Not all who wander are lost

#6 Pres

Pres

    Retired Art Teacher

  • Moderators
  • 3,179 posts
  • LocationCentral, PA

Posted 11 June 2013 - 12:18 PM

I tend to incise deeper lines than is typical for sgraffito, and there's definitely a 'sweet spot'. I like things a little harder than is typically referred to as 'cheese hard'- hard enough to yield sharp, clean, flowing lines without the tool catching or any fracturing in the clay.

It's a surprisingly finite range... but glorious when you find it.


I like to carve bamboo chopsticks into sgraffito tools. They are cheap, I can have several different shapes, and they leave a smooth mark in leather hard clay.
Simply retired teacher, not dead, living the dream. on and on and. . . . on. . . . http://picworkspottery.blogspot.com/

#7 Benzine

Benzine

    Socratic Potter

  • Members
  • PipPipPip
  • 2,430 posts
  • LocationThe Hawkeye State

Posted 11 June 2013 - 12:55 PM

I use dental tools, for some of my sgraffito, as well as my detailed carving. They are small, and even though when I get them, they are worn for their intended purpose, they are more than sharp enough to cleanly carve into clay.
"Anything worth believing, is worth questioning"

#8 Kohaku

Kohaku

    Huffing cobalt over a Raku kiln

  • Members
  • PipPipPip
  • 331 posts
  • LocationMoscow, Idaho

Posted 11 June 2013 - 03:17 PM

I use dental tools, for some of my sgraffito, as well as my detailed carving. They are small, and even though when I get them, they are worn for their intended purpose, they are more than sharp enough to cleanly carve into clay.


... and where does one get used dental tools?
Not all who wander are lost

#9 Pres

Pres

    Retired Art Teacher

  • Moderators
  • 3,179 posts
  • LocationCentral, PA

Posted 11 June 2013 - 03:23 PM


I use dental tools, for some of my sgraffito, as well as my detailed carving. They are small, and even though when I get them, they are worn for their intended purpose, they are more than sharp enough to cleanly carve into clay.


... and where does one get used dental tools?


Check with your local dentists. I also find them at the local large hardware surplus store. It seems that they are popular for a lot of uses like soldering and carving, cleaning tools etc.
Simply retired teacher, not dead, living the dream. on and on and. . . . on. . . . http://picworkspottery.blogspot.com/

#10 jrgpots

jrgpots

    The hands can express the soul

  • Members
  • PipPipPip
  • 806 posts
  • LocationHurricane, Utah

Posted 11 June 2013 - 04:39 PM



I use dental tools, for some of my sgraffito, as well as my detailed carving. They are small, and even though when I get them, they are worn for their intended purpose, they are more than sharp enough to cleanly carve into clay.


... and where does one get used dental tools?


Check with your local dentists. I also find them at the local large hardware surplus store. It seems that they are popular for a lot of uses like soldering and carving, cleaning tools etc.



Leather working and tooling shops also sell them. as well as many stamps, cutters, etc.

#11 Benzine

Benzine

    Socratic Potter

  • Members
  • PipPipPip
  • 2,430 posts
  • LocationThe Hawkeye State

Posted 11 June 2013 - 10:38 PM


I use dental tools, for some of my sgraffito, as well as my detailed carving. They are small, and even though when I get them, they are worn for their intended purpose, they are more than sharp enough to cleanly carve into clay.


... and where does one get used dental tools?





I use dental tools, for some of my sgraffito, as well as my detailed carving. They are small, and even though when I get them, they are worn for their intended purpose, they are more than sharp enough to cleanly carve into clay.


... and where does one get used dental tools?



Check with your local dentists. I also find them at the local large hardware surplus store. It seems that they are popular for a lot of uses like soldering and carving, cleaning tools etc.






I use dental tools, for some of my sgraffito, as well as my detailed carving. They are small, and even though when I get them, they are worn for their intended purpose, they are more than sharp enough to cleanly carve into clay.


... and where does one get used dental tools?


Check with your local dentists. I also find them at the local large hardware surplus store. It seems that they are popular for a lot of uses like soldering and carving, cleaning tools etc.



Leather working and tooling shops also sell them. as well as many stamps, cutters, etc.


Or, you could just be married to a dental assistant.......
"Anything worth believing, is worth questioning"

#12 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,359 posts
  • LocationRed Lodge, Montana

Posted 14 June 2013 - 10:37 AM

I used a porcupine quill on this one. Cone 5 dark clay with porcelain slip on top. blue slip brushed on.
http://ceramicartsda...wimage&img=2213

Cheese hard is the way to go.
Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#13 oldlady

oldlady

    single firing an electric kiln to cone 6

  • Members
  • PipPipPip
  • 3,452 posts
  • Locationharpers ferry west va and pinellas park fl

Posted 14 June 2013 - 07:15 PM

I used a porcupine quill on this one. Cone 5 dark clay with porcelain slip on top. blue slip brushed on.
http://ceramicartsda...wimage&img=2213

Cheese hard is the way to go.
Marcia





for some reason i cannot see the link. the page that comes up is form CAD saying i am not logged in. can't get around it. have been logged in almost all day trying to get these DA^%(*%^m pictures in.
"putting you down does not raise me up."

#14 Benzine

Benzine

    Socratic Potter

  • Members
  • PipPipPip
  • 2,430 posts
  • LocationThe Hawkeye State

Posted 14 June 2013 - 09:29 PM


I used a porcupine quill on this one. Cone 5 dark clay with porcelain slip on top. blue slip brushed on.
http://ceramicartsda...wimage&img=2213

Cheese hard is the way to go.
Marcia





for some reason i cannot see the link. the page that comes up is form CAD saying i am not logged in. can't get around it. have been logged in almost all day trying to get these DA^%(*%^m pictures in.


I have had the same issue, with Marcia's link, and at least one other. I even tried logging in again, to no avail.
"Anything worth believing, is worth questioning"

#15 Pugaboo

Pugaboo

    Lifetime artist 3rd year potter

  • Members
  • PipPipPip
  • 1,037 posts
  • LocationHelen, GA

Posted 14 June 2013 - 10:11 PM

I too am having this issue with clicking on links. Message says I do not have permission to do this action and I should log in so I can do so... Re-logging is of no help still can't get the links to work. What am I doing wrong?

Terry
The world is but a canvas to the imagination - Henry David Thoreau

#16 Kohaku

Kohaku

    Huffing cobalt over a Raku kiln

  • Members
  • PipPipPip
  • 331 posts
  • LocationMoscow, Idaho

Posted 14 June 2013 - 10:19 PM

I too am having this issue with clicking on links. Message says I do not have permission to do this action and I should log in so I can do so... Re-logging is of no help still can't get the links to work. What am I doing wrong?

Terry


Glad it's not just me.
Not all who wander are lost

#17 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,359 posts
  • LocationRed Lodge, Montana

Posted 15 June 2013 - 02:05 AM

Could be the incredibly SLOW wifi at my hotels.
maybe it doesn't all get included. The link is to my gallery, made in France album ..there is a square plaque in there with sgraffito.
I will be back home tomorrow night.
Should not have issues after that.
Ciao.
I am ready to be home.
Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#18 annekat

annekat

    Advanced Member

  • Members
  • PipPipPip
  • 44 posts
  • LocationOlympia, Washington

Posted 17 June 2013 - 02:13 PM

Me, too, having the problem..... looking forward to seeing your pics when you get back, Marcia!
Anne

#19 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,359 posts
  • LocationRed Lodge, Montana

Posted 17 June 2013 - 03:56 PM

This is the sgrafitto piece from my gallery

http://ceramicartsda...wimage&img=2213

I am home now. Tis was a dark clay with a porcelain slip applied. Then drawn using a porcupine quill. It is a street scene outside the studio in the old medieval part of Vallauris, France.

AIR Vallauris is where I did a residency last October. It worked when I clicked on it. Let me know if it is working. Got home last night from the Tuscany Tour III. It was really a great group. Nice people. All went smoothly except for some twisted ankles. So much to see looking up, people walked off curbs.


Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#20 Celia UK

Celia UK

    Advanced Member

  • Members
  • PipPipPip
  • 447 posts
  • LocationCambridge, England

Posted 17 June 2013 - 04:18 PM

This is the sgrafitto piece from my gallery

http://ceramicartsda...wimage&img=2213

I am home now. Tis was a dark clay with a porcelain slip applied. Then drawn using a porcupine quill. It is a street scene outside the studio in the old medieval part of Vallauris, France.

AIR Vallauris is where I did a residency last October. It worked when I clicked on it. Let me know if it is working. Got home last night from the Tuscany Tour III. It was really a great group. Nice people. All went smoothly except for some twisted ankles. So much to see looking up, people walked off curbs.


Marcia






0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users