Hi - new member and fairly new to ceramics - I am wondering if it is possible to use black iron oxide on greenware as a wash, without wiping away, and to bisque fire pieces this way. If so, how thin of a wash must I use?

Thank you

#2 SmartsyArtsy

SmartsyArtsy

    Chris Seminara

  • Members
  • PipPipPip
  • 182 posts
  • LocationPNW

Posted 27 May 2013 - 02:47 AM

The general answer is Yes. But I advise you to add a flux, maybe Frit 3124, 3110 to help . As to how much/thin to apply there are some questions: Which iron oxide are you using? What color clay are you using? What cone do you expect to fire? Higher temp will burn more of it out.

#3 barb9000

barb9000

    Newbie

  • Members
  • Pip
  • 3 posts

Posted 27 May 2013 - 09:18 AM

Thank you Chris - It is a black iron oxide, on soldate 60 clay. I am more concerned about whether it is safe vs. end result. It won't cause the clay to explode or anything, will it?

#4 SmartsyArtsy

SmartsyArtsy

    Chris Seminara

  • Members
  • PipPipPip
  • 182 posts
  • LocationPNW

Posted 27 May 2013 - 08:32 PM

No explosions! You might have to test color depth a bit. I add less frit than oxide, although others add equal parts. Have fun.

#5 barb9000

barb9000

    Newbie

  • Members
  • Pip
  • 3 posts

Posted 27 May 2013 - 10:18 PM

Thank you again Chris!

#6 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,361 posts
  • LocationRed Lodge, Montana

Posted 28 May 2013 - 10:26 AM

You can use iron oxide easier as a wash on bisque if you are trying to accent texture.
The iron stays in the crevices after sponging over the surface. Using it at the greenware
stage would wash away the texture. Not sure what your goal is.

Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#7 Biglou13

Biglou13

    Advanced Member

  • Members
  • PipPipPip
  • 1,258 posts
  • LocationNorth Florida

Posted 28 May 2013 - 01:00 PM

What the big difference with RIO. And. BIO. My RIO washes usually turn out black.

LEC potttery  on facebook, instagram

 

The true sign of intelligence is not knowledge but imagination.
-Albert Einstein


#8 Pres

Pres

    Retired Art Teacher

  • Moderators
  • 3,180 posts
  • LocationCentral, PA

Posted 28 May 2013 - 01:31 PM

You can use iron oxide easier as a wash on bisque if you are trying to accent texture.
The iron stays in the crevices after sponging over the surface. Using it at the greenware
stage would wash away the texture. Not sure what your goal is.

Marcia


Marcia, I have sprayed iron oxide on heavily textured buff colored clays, and then lightly sanded them with a scruff pad to bring up the high areas. I spray because I do not want to soften the greenware texture with the brushing. This works well for a lot of things especially when using a light body underneath. Now I am trying the same thing with a darker body under, and a white slip over top.
Simply retired teacher, not dead, living the dream. on and on and. . . . on. . . . http://picworkspottery.blogspot.com/

#9 Mart

Mart

    Advanced Member

  • Members
  • PipPipPip
  • 283 posts

Posted 28 May 2013 - 01:38 PM

What the big difference with RIO. And. BIO. My RIO washes usually turn out black.


Red iron(III) oxide - Fe2O3
Black iron(II) oxide - FeO

At high temperatures, Fe2O3 starts to break down so O and F take off and you are left with the FeO
In oxidation, this is how you get those cool "oil spots" happening on the glaze where Fe2O3 is converting and free O drags F to the surface and leaves it there.
Someone can probably get you more detailed description of the process.

#10 davidh

davidh

    Newbie

  • Members
  • Pip
  • 2 posts
  • Locationcalifornia

Posted 29 May 2013 - 12:16 PM

The general answer is Yes. But I advise you to add a flux, maybe Frit 3124, 3110 to help . As to how much/thin to apply there are some questions: Which iron oxide are you using? What color clay are you using? What cone do you expect to fire? Higher temp will burn more of it out.

Chris, why do you add flux and why frit? I thought iron oxide was a flux in itself. Would you use it whether it was greenware or bisk?
thanks david




#11 loveceramics85

loveceramics85

    Member

  • Members
  • PipPip
  • 14 posts

Posted 13 June 2013 - 04:59 AM


The general answer is Yes. But I advise you to add a flux, maybe Frit 3124, 3110 to help . As to how much/thin to apply there are some questions: Which iron oxide are you using? What color clay are you using? What cone do you expect to fire? Higher temp will burn more of it out.

Chris, why do you add flux and why frit? I thought iron oxide was a flux in itself. Would you use it whether it was greenware or bisk?
thanks david





#12 loveceramics85

loveceramics85

    Member

  • Members
  • PipPip
  • 14 posts

Posted 13 June 2013 - 05:06 AM

The general answer is Yes. But I advise you to add a flux, maybe Frit 3124, 3110 to help . As to how much/thin to apply there are some questions: Which iron oxide are you using? What color clay are you using? What cone do you expect to fire? Higher temp will burn more of it out.


hi Chris what happens if i do not use a flux or a frit to the oxide to my work and would it make a different if i was applying it to a bisque or green ware work????

#13 oldlady

oldlady

    single firing an electric kiln to cone 6

  • Members
  • PipPipPip
  • 3,458 posts
  • Locationharpers ferry west va and pinellas park fl

Posted 15 June 2013 - 12:58 PM

i am not a technical person, just one who goes by experience. you seem to have an underlying lack of knowledge about the whole process if you originally thought something would explode if you covered it in a wash. a wash as i define it is simply wet oxide you apply by some means to a pot whether green or bisque. the oxide alone will become dust if you handle it after the application. these people trying to help you are suggesting some way of preventing that dusting off of the pot and the color staying more firmly fixed in place.

what is it you are trying to do? if you can formulate the question you may get better answers.
"putting you down does not raise me up."

#14 Benzine

Benzine

    Socratic Potter

  • Members
  • PipPipPip
  • 2,430 posts
  • LocationThe Hawkeye State

Posted 15 June 2013 - 04:20 PM

You can use iron oxide easier as a wash on bisque if you are trying to accent texture.
The iron stays in the crevices after sponging over the surface. Using it at the greenware
stage would wash away the texture. Not sure what your goal is.

Marcia


This is how, I've always used oxides. It's a great effect.
"Anything worth believing, is worth questioning"

#15 Celia UK

Celia UK

    Advanced Member

  • Members
  • PipPipPip
  • 447 posts
  • LocationCambridge, England

Posted 18 December 2013 - 02:19 AM

I am using oxides (usually copper oxide/carbonate) to highlight some parts of my pots, by masking where I don't want this, and spraying the oxide solution lightly with an airbrush. I'm aiming for a subtle 'blush' within the transparent glaze. A few questions to help me perfect the process! I particularly want to avoid the oxides moving on to areas I want to remain white, and want a subtle effect overall.

- does it make any difference whether the oxide is under or over the transparent glaze?
- if it's under, can I fire it on, to prevent it moving when covered by the glaze?
- If so, what is the lowest temperature that will achieve this?
- alternatively, could I add the oxide to some of the transparent glaze (instead of using in wash form), spray or brush this, remove masking and spray over the whole piece - would the oxide still break through?

Any advice would be most welcome. Thank you.

#16 weeble

weeble

    Advanced Member

  • Members
  • PipPipPip
  • 121 posts
  • LocationOregon Coast

Posted 19 December 2013 - 04:56 AM

I've been using copper carb in a way that might answer some of your questions.  I mix the copper carb with a white terra sig just because its a handy way to stick the stuff, copper carb seems to wipe off a lot easier than RIO and mang.diox.  I apply this mix to a textured bisqued piece, then wipe it off the areas I want the base clay color to show then put my transparent over and glaze fire. This gives a nice green with a wide range of light and dark areas.  Adding the copper carb to the glaze directly gives a much more uniform look, less textured, so its not what I want.  It makes a nice green glaze if that's what you want though.  Some of the carb burns out so I don't worry about getting it all off.  Applying over the glaze seems to be a bit more irregular on what burns out. As I'm looking to emphasize the texture, this works much better.  A thicker layer of glaze = more movement of the color.  Sometimes I'll re-bisque to lock the copper carb on before glazing, sometimes not.  Its a time and patience thing!

 

Attached File  1bon4.jpg   66.43KB   45 downloads

 

Here I wiped almost all the copper carb off the raised surface and used a semi-transparent satin white over the copper carb. then went back in and added more carb on the lip of the pot.  


Maryjane Carlson

Whistling Fish Pottery

#17 Celia UK

Celia UK

    Advanced Member

  • Members
  • PipPipPip
  • 447 posts
  • LocationCambridge, England

Posted 19 December 2013 - 05:17 AM

Thanks Maryjane - that will be another series of tests for me

Texture isn't the thing with the particular pieces in question, but I do also do textured bowls, so I can store this up for the future!

Attached is a picture of one bisqued bowl which I have airbrushed with copper carbonate (was awaiting for advice before deciding whether to do a 2nd bisque before glazing!) so you can see what I'm on about and another finished piece with the effect I'm after (I made this way back and can't remember how I went about it!)
No idea why my photos turn round when attached - perhaps it's an ipad thing!Attached File  image.jpg   95.82KB   28 downloadsAttached File  image.jpg   89.7KB   18 downloads

#18 weeble

weeble

    Advanced Member

  • Members
  • PipPipPip
  • 121 posts
  • LocationOregon Coast

Posted 19 December 2013 - 08:21 PM

I normally sponge or brush my glaze on, but I bet if you're spraying you'll be fine just going with the one bisque.  With brushing though, the copper carb was lifting, which is why I started using a terra sig base and often do the second bisque. You're just going to have to do some tests to see what the glaze/copper carb combination do.  


Maryjane Carlson

Whistling Fish Pottery

#19 Celia UK

Celia UK

    Advanced Member

  • Members
  • PipPipPip
  • 447 posts
  • LocationCambridge, England

Posted 30 July 2014 - 09:21 AM

Thanks for all the info, just one question not yet answered for me.
If I spray oxide on to bisque and want to refire to fix it before glazing - what temperature will fix it?
In the future I think I'll spray on to greenware, but currently I have a few pieces already bisqued & don't want the oxide to move at all.

#20 Babs

Babs

    Advanced Member

  • Members
  • PipPipPip
  • 2,077 posts

Posted 30 July 2014 - 05:57 PM

I don't think you need to add frit to an oxide you're using as a wash.

Firing it on a bisque to set it for glazing seems an extra step and will, yes keep it in place during the glazing process but not during the glaze firing, this would depend on the nature of hte glaze. Some people merely spray a starch or soft drink onto the area to set it before glazing without the extra firing.

On white bodies I prefer to put the oxide ono greenware as onto a bisque seems to colour the clay body.

But if scouring any dry clay use appropriate safety measures.