Posted 22 May 2013 - 03:35 AM

I'm going to start working with cone 6 porcelain.....my friends are great artists, and I dont have the time to learn another craft at the second. Can anyone recommend me a company that will print out my friends designs? I would like to do the decal, then put a clear glaze over it. Is this how it works? Thanks....Justin

#2 oldlady

oldlady

    single firing an electric kiln to cone 6

  • Members
  • PipPipPip
  • 3,449 posts
  • Locationharpers ferry west va and pinellas park fl

Posted 22 May 2013 - 03:51 PM

what country are you living in? your post might get answers if you remove the word "cheap" from it.

what you are describing sounds like a typical china production company ( think of your mom's dishes) operation. maybe you could contact one of them.
"putting you down does not raise me up."

#3 Mark C.

Mark C.

    Advanced Member

  • Members
  • PipPipPip
  • 6,304 posts
  • LocationNear Arcata Ca-redwood rain forest

Posted 23 May 2013 - 01:10 AM

The decals I have been around and it was years ago -you applied over a fired glaze then fired to cone 017 if I recall. I do not recall cheap in any ceramic process unless you mean pit firing.
You can print your own decals with the right stuff-Google may be of help on this-there have been a few articles in the ceramic rags on this.
Mark
Mark Cortright
www.liscomhillpottery.com

#4 AtomicAxe

AtomicAxe

    Skilled Mud Bug

  • Members
  • PipPipPip
  • 195 posts
  • LocationAmarillo, TX

Posted 23 May 2013 - 10:14 AM

Just make your own. There are tons of ways, easiest being a litho process.

#5 Bobg

Bobg

    Advanced Member

  • Members
  • PipPipPip
  • 83 posts
  • Locationsoutheastern WA

Posted 23 May 2013 - 10:30 AM

Wasn't there someone that's a member here was using a laser printer to make decals?

Bob