Will firing make imperfections more or less noticeable?

Recommended Posts

futurebird    1

I'm making unglazed-ware-- specifically yixing teapots. I won't get to fire them for a very long time. Which is fine, I nee to practice.

 

But I wonder what firing will do.

 

How will it change burnishing?

 

ttt2.jpg

Is burnishing worth it?

 

Will it tone down imperfections or heighten them?

 

My goal here is *perfection* for it to look almost machine-made. I'm always looking for way to improve symmetry and smoothness.

Share this post


Link to post
Share on other sites
TJR    359

Futurebird;

Yixing teapots are burnished and are unglazed. Purchase or make some terra sigilatta.[look it up].Brush it on the leather hard pot. Burnish with a spoon or a stone.

Then you will smooth out some imperfections.

TJR.

Share this post


Link to post
Share on other sites
OffCenter    82

I'm making unglazed-ware-- specifically yixing teapots. I won't get to fire them for a very long time. Which is fine, I nee to practice.

 

But I wonder what firing will do.

 

How will it change burnishing?

 

ttt2.jpg

 

Is burnishing worth it?

 

Will it tone down imperfections or heighten them?

 

My goal here is *perfection* for it to look almost machine-made. I'm always looking for way to improve symmetry and smoothness.

 

 

I've seen but haven't read your other posts about making these teapots, so sorry about asking questions that you've already answered elsewhere and I'm too lazy to look up, but: These are handbuilt, right? Are these your first teapots? (I like them.) Since I don't know how high they will be fired, I don't know if burnishing is worth it, but am guessing that it isn't.

 

Jim

Share this post


Link to post
Share on other sites
TJR    359

Burnishing is a low fire technique, never meant to be fired higher than cone06.Neil and Jim are correct. It will burn off in higher temperatures.

TJR.

Share this post


Link to post
Share on other sites
futurebird    1

Burnishing is a low fire technique, never meant to be fired higher than cone06.Neil and Jim are correct. It will burn off in higher temperatures.

TJR.

 

 

How do the masters get their pots so shiny? I know some are polished after firing-- or coated in tea after years of use... but even new pots seem to shine...

 

18th+century+Yixing+teapots.jpg

 

The idea of using slip to burnish in interesting, but I wonder of it is done that way in China. This clay has been worked for 600 years I want to learn the traditional way before I modify it

 

I was told that you polish the pot with ox horn... so that's what I tried to do.

Share this post


Link to post
Share on other sites
futurebird    1

 

 

I've seen but haven't read your other posts about making these teapots, so sorry about asking questions that you've already answered elsewhere and I'm too lazy to look up, but: These are handbuilt, right? Are these your first teapots? (I like them.) Since I don't know how high they will be fired, I don't know if burnishing is worth it, but am guessing that it isn't.

 

Jim

 

 

 

These are my 12th and 13th hand built pots you don't want to see the first one. laugh.gif

Share this post


Link to post
Share on other sites
Marcia Selsor    1,301

After applying terra sig to a bone dry piece, I buff it with a soft cloth. I never liked the streaks created by using a hard tool to burnish.

 

Marcia

Share this post


Link to post
Share on other sites
Chris Campbell    1,088

Just taking a stab at it ... But a lovely terra sig will leave that kind of a surface and survives firing ... At least mine have to cone 6.

Share this post


Link to post
Share on other sites
JBaymore    1,432

Maybe make a terra sig out of the Yixing clay body you are using. Not hard to do. Google it.

 

best,

 

.............john

Share this post


Link to post
Share on other sites
JLowes    28

It is my understanding that Yixing clay (zisha clay) unique to Yixing, and thus maybe the shine comes from the properties of that clay, rather than burnishing or terra sig. I think I read that it has iron, quartz and mica in the clay, and is running out. Get those teapots while you still can.

 

John

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×