I'm making unglazed-ware-- specifically yixing teapots. I won't get to fire them for a very long time. Which is fine, I nee to practice.

But I wonder what firing will do.

How will it change burnishing?

Posted Image

Is burnishing worth it?

Will it tone down imperfections or heighten them?

My goal here is *perfection* for it to look almost machine-made. I'm always looking for way to improve symmetry and smoothness.

www.futurebird.com

#2 TJR

TJR

    Advanced Member

  • Members
  • PipPipPip
  • 1,821 posts
  • LocationWinnipeg,Manitoba,Canada

Posted 16 May 2013 - 08:12 AM

Futurebird;
Yixing teapots are burnished and are unglazed. Purchase or make some terra sigilatta.[look it up].Brush it on the leather hard pot. Burnish with a spoon or a stone.
Then you will smooth out some imperfections.
TJR.

#3 OffCenter

OffCenter

    Advanced Member

  • Members
  • PipPipPip
  • 1,372 posts

Posted 16 May 2013 - 08:17 AM

I'm making unglazed-ware-- specifically yixing teapots. I won't get to fire them for a very long time. Which is fine, I nee to practice.

But I wonder what firing will do.

How will it change burnishing?

Posted Image

Is burnishing worth it?

Will it tone down imperfections or heighten them?

My goal here is *perfection* for it to look almost machine-made. I'm always looking for way to improve symmetry and smoothness.


I've seen but haven't read your other posts about making these teapots, so sorry about asking questions that you've already answered elsewhere and I'm too lazy to look up, but: These are handbuilt, right? Are these your first teapots? (I like them.) Since I don't know how high they will be fired, I don't know if burnishing is worth it, but am guessing that it isn't.

Jim
E pur si muove.

"But it does move," said Galileo under his breath.

#4 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 4,830 posts
  • LocationGrayslake, IL

Posted 16 May 2013 - 08:19 AM

A highly polished surface will dull when it is fired.

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

[email protected]


#5 TJR

TJR

    Advanced Member

  • Members
  • PipPipPip
  • 1,821 posts
  • LocationWinnipeg,Manitoba,Canada

Posted 16 May 2013 - 08:25 AM

Burnishing is a low fire technique, never meant to be fired higher than cone06.Neil and Jim are correct. It will burn off in higher temperatures.
TJR.

#6 futurebird

futurebird

    Advanced Member

  • Members
  • PipPipPip
  • 46 posts

Posted 16 May 2013 - 09:10 AM

Burnishing is a low fire technique, never meant to be fired higher than cone06.Neil and Jim are correct. It will burn off in higher temperatures.
TJR.


How do the masters get their pots so shiny? I know some are polished after firing-- or coated in tea after years of use... but even new pots seem to shine...

Posted Image

The idea of using slip to burnish in interesting, but I wonder of it is done that way in China. This clay has been worked for 600 years I want to learn the traditional way before I modify it

I was told that you polish the pot with ox horn... so that's what I tried to do.
www.futurebird.com

#7 futurebird

futurebird

    Advanced Member

  • Members
  • PipPipPip
  • 46 posts

Posted 16 May 2013 - 09:20 AM

I've seen but haven't read your other posts about making these teapots, so sorry about asking questions that you've already answered elsewhere and I'm too lazy to look up, but: These are handbuilt, right? Are these your first teapots? (I like them.) Since I don't know how high they will be fired, I don't know if burnishing is worth it, but am guessing that it isn't.

Jim



These are my 12th and 13th hand built pots you don't want to see the first one. Posted Image
www.futurebird.com

#8 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,150 posts
  • LocationRed Lodge, Montana

Posted 16 May 2013 - 09:24 AM

After applying terra sig to a bone dry piece, I buff it with a soft cloth. I never liked the streaks created by using a hard tool to burnish.

Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#9 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,074 posts
  • LocationRaleigh, NC

Posted 16 May 2013 - 03:20 PM

Just taking a stab at it ... But a lovely terra sig will leave that kind of a surface and survives firing ... At least mine have to cone 6.

Chris Campbell

Contemporary Fine Colored Porcelain
www.ccpottery.com

 

TRY ... FAIL ... LEARN ... REPEAT

" ... If a sufficient number of people are different, no one has to be normal"
Fredrick Bachman


#10 JBaymore

JBaymore

    Moderator

  • Moderators
  • 4,133 posts
  • LocationWilton, NH USA

Posted 16 May 2013 - 04:20 PM

Maybe make a terra sig out of the Yixing clay body you are using. Not hard to do. Google it.

best,

.............john

John Baymore
Professor of Ceramics; New Hampshire Insitute of Art

Guest Professor, Wuxi Institute of Arts and Science, Yixing, China

Former President and Past President; Potters Council
 

http://www.JohnBaymore.com

http://www.nhia.edu/...ty/john-baymore


#11 JLowes

JLowes

    Clay Doodler

  • Members
  • PipPipPip
  • 266 posts
  • LocationAtlanta Georgia area

Posted 16 May 2013 - 08:49 PM

It is my understanding that Yixing clay (zisha clay) unique to Yixing, and thus maybe the shine comes from the properties of that clay, rather than burnishing or terra sig. I think I read that it has iron, quartz and mica in the clay, and is running out. Get those teapots while you still can.

John