I have a question concerning safety of pottery dishes: Is it safe to drink from dishes with crakled glaze? (this one http://www.ebay.com/...n-/260368966974 ). Thanks for your answers

#2 AtomicAxe

AtomicAxe

    Skilled Mud Bug

  • Members
  • PipPipPip
  • 195 posts
  • LocationAmarillo, TX

Posted 13 May 2013 - 02:24 PM

I have a question concerning safety of pottery dishes: Is it safe to drink from dishes with crakled glaze? (this one http://www.ebay.com/...n-/260368966974 ). Thanks for your answers


that isn't a crackled glaze, that is a simple clear with a copper green liner and iron oxide brushing. I see little to no crazing in that glaze to indicate it would allow liquid through it.

As far as crackle glazes go ... http://www.gtp.com.a...ages/CV-810.jpg ... the important question is ... "is this a stoneware piece?" since you need to know if it reached a temperature high enough to stop absorbing liquids. From what I've seen on that ebay listing ... who knows.

#3 DavidDivad

DavidDivad

    Newbie

  • Members
  • Pip
  • 2 posts

Posted 14 May 2013 - 01:20 AM


I have a question concerning safety of pottery dishes: Is it safe to drink from dishes with crakled glaze? (this one http://www.ebay.com/...n-/260368966974 ). Thanks for your answers


that isn't a crackled glaze, that is a simple clear with a copper green liner and iron oxide brushing. I see little to no crazing in that glaze to indicate it would allow liquid through it.

As far as crackle glazes go ... http://www.gtp.com.a...ages/CV-810.jpg ... the important question is ... "is this a stoneware piece?" since you need to know if it reached a temperature high enough to stop absorbing liquids. From what I've seen on that ebay listing ... who knows.




I posted that link to show what kind of cup I was talking about. And I should probably use “cracked“ instead of “crackled“ - I dropped it once. But liquid isnt leaking or sth.

They bake the bowl at 1230-1250℃, they paint the bowl and then they bake it at 700-800℃ ( http://remiojapan.co...i-mino-pottery/ )



At least it has more wabi-sabi look, but still..... Posted Image