shayes

Silver glaze/ ceramic glaze sealer

Recommended Posts

shayes    1

I received an order for a special wedding present. A ceramic champagne holder (vase) and champagne glasses, colors are red, white and silver. I was able to achieve a very nice white and red, but am having a really hard time with silver! I fired my piece at cone 9, so there wasn't any options of a silver high fire glaze. I used a silver sharpie pen to create a thin line, which looks really nice, but comes off very easily with water. The small silver accent line is on the outside of the pieces and doesn't necessarily have to be food safe, just permanent!

 

Anyone know of a permanent clear sealer I can apply on top of glaze??

 

Or a permanent silver paint that will stick on glaze????

Share this post


Link to post
Share on other sites
AtomicAxe    19

Nothing you can do with a silver sharpie ... it's just a dye with something to stick ... you can try to clear coat it with a clear spray paint ... but the acetone and xylene in spray paint will dissolve it.

 

That being said ...

 

 

 

Why did you not think to silver leaf the job? http://www.gildedplanet.com/howtogoldleaf.asp

Share this post


Link to post
Share on other sites
shayes    1

I've never tried of even heard of silver leaf, still learning! Is it possible to try this technique on top of an already fired and glazed surface?

Share this post


Link to post
Share on other sites
Pompots    4

you might want to try pebeo porcelaine 150 those are enamels that fire in your house oven at 325F for 40 minutes and they are as permanent as glaze. they are really strong and actually dishwasher safe once they have been fired. they have all kinds of metallic colors.

Share this post


Link to post
Share on other sites
Marcia Selsor    1,301

Why not use a silver luster?

It looks better than silver paint. It may not be dish washer safe.

 

You fire it to ^018-020.

 

Marcia

Share this post


Link to post
Share on other sites
shayes    1

you might want to try pebeo porcelaine 150 those are enamels that fire in your house oven at 325F for 40 minutes and they are as permanent as glaze. they are really strong and actually dishwasher safe once they have been fired. they have all kinds of metallic colors.

 

 

wow, just looked into this and purchased a few colors on amazon. i'm trying both the pebeo porcelaine 150 pens and paint. seems to have great reviews and as long as it works, this is exactly what i'm looking for! really appreciate your advice!

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×