Posted 12 May 2013 - 01:27 PM

I started an additional subject on sawdust burners which didn't quite fit into the wood-fired forced air topic.
Lowell Baker has been working on these for a long time. He gives workshops all over the place. Here is a Youtube on his sawdust injected burner.

Marcia


Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#2 Biglou13

Biglou13

    Advanced Member

  • Members
  • PipPipPip
  • 1,258 posts
  • LocationNorth Florida

Posted 12 May 2013 - 06:54 PM

I started an additional subject on sawdust burners which didn't quite fit into the wood-fired forced air topic.
Lowell Baker has been working on these for a long time. He gives workshops all over the place. Here is a Youtube on his sawdust injected burner.

Marcia



Very very cool. Brilliant.

I had thoughts of using sawdust. But not so technical...

Is he still doing workshops?

Have you seen pottery from sawdust burner, any similarities to wood fire?

Big thanks for the info.

LEC potttery  on facebook, instagram

 

The true sign of intelligence is not knowledge but imagination.
-Albert Einstein


#3 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,150 posts
  • LocationRed Lodge, Montana

Posted 13 May 2013 - 06:13 AM

Yes. Google him.
He was teaching in Alabama. He may be part of the Alabama Clay Fest in Feb.

Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#4 Biglou13

Biglou13

    Advanced Member

  • Members
  • PipPipPip
  • 1,258 posts
  • LocationNorth Florida

Posted 20 May 2013 - 09:20 PM

Anyone have experience, with sawdust burner?

LEC potttery  on facebook, instagram

 

The true sign of intelligence is not knowledge but imagination.
-Albert Einstein


#5 Biglou13

Biglou13

    Advanced Member

  • Members
  • PipPipPip
  • 1,258 posts
  • LocationNorth Florida

Posted 23 May 2013 - 01:49 PM

Anyone have experience, with sawdust burner?


Another lowell baker sawdust burner. Video.


LEC potttery  on facebook, instagram

 

The true sign of intelligence is not knowledge but imagination.
-Albert Einstein


#6 Wyndham

Wyndham

    Advanced Member

  • Members
  • PipPipPip
  • 486 posts
  • LocationSeagrove NC

Posted 25 May 2013 - 09:45 AM

Back in the mid 1970's there was a Cedar mill in Texas that I worked. We ground up dry Cedar stumps into sawdust and extracted the oil with a steam evaporation and cooling system(a still).
The waste sawdust was burned to heat the boiler that produced the steam.
It had a firebox that sawdust was dragged by chain into a hopper over the firebox. a forced air system with 6- 1in tubes, 3 on a side. These were used to "fluff up" the sawdust and provide some air and a main blower pushed the flame into the boiler box that heated the water to steam.

Long before I knew what a celadon glaze was, I found a green glaze slag drip from the iron lip under the boiler box where the flame entered.

I think this design could serve as a model for a sawdust fired kiln using squirrel cage blowers and a distribute or manifold air system with a hopper feeder for the sawdust.

Wyndham