Big Lou I was just doing some research on that subject, I have a project that calls for plaster of paris I always have a bag of pottery plaster around and it's a lot cheaper than plaster of paris. Around here pottery plaster is 7 dollars for 50 lbs. and 20 for 25 lbs plaster of paris. Pottery plaster is harder more durable and less absorbent and is considered a higher quality plaster. For a hump mold I would go for the pottery plaster for durability and less absorbent. Denice

Share this post


Link to post
Share on other sites

USG#1. Is only 20.50/ 50# bag plus a 45 min drive. And the danger to wallet for going to toy store. (US gypsum)

 

 

$ 15/25# plaster o Paris. @home depot.

 

(What's Paris got to do wit it?)

Share this post


Link to post
Share on other sites

Home depot plaster is ment for softer applications like patching or covering walls, stuff like that ... as such it tends to not be nice for things like slip molds ... but really ... if you don't abuse the snot out of it you shouldn't have to worry anyways. I have a plaster mold that has to be 9 years old, just as nice as the first day I made it. Oh and if you are going to make a big mold ... put some fiber in it, it helps.

Share this post


Link to post
Share on other sites

Home depot plaster is ment for softer applications like patching or covering walls, stuff like that ... as such it tends to not be nice for things like slip molds ... but really ... if you don't abuse the snot out of it you shouldn't have to worry anyways. I have a plaster mold that has to be 9 years old, just as nice as the first day I made it. Oh and if you are going to make a big mold ... put some fiber in it, it helps.

 

 

Metamucil?

 

What do you use for fiber?

 

It's only 15 ish inches diameter ish. Read about hardware cloth and scrim cloth.

 

I have a few sheets of drywall sanding screen I'm going reinforce with.

 

Thanks all for the 411

 

PS. Large gypsum deposit at Montmartre in Paris led "calcined gypsum" (roasted gypsum or gypsum plaster) to be commonly known as "plaster of Paris". Ala Webster/Wikipedia.......

Share this post


Link to post
Share on other sites

For casting, #1 plaster is the best. For hump molds, plaster of Paris should work just fine. I have seen people use carved closed-cell foam for hump molds, if you want cheap and carveable.

Share this post


Link to post
Share on other sites

Home depot plaster is ment for softer applications like patching or covering walls, stuff like that ... as such it tends to not be nice for things like slip molds ... but really ... if you don't abuse the snot out of it you shouldn't have to worry anyways. I have a plaster mold that has to be 9 years old, just as nice as the first day I made it. Oh and if you are going to make a big mold ... put some fiber in it, it helps.

 

 

Metamucil?

 

What do you use for fiber?

 

It's only 15 ish inches diameter ish. Read about hardware cloth and scrim cloth.

 

I have a few sheets of drywall sanding screen I'm going reinforce with.

 

Thanks all for the 411

 

PS. Large gypsum deposit at Montmartre in Paris led "calcined gypsum" (roasted gypsum or gypsum plaster) to be commonly known as "plaster of Paris". Ala Webster/Wikipedia.......

 

 

Sorry, I thought I should be more specific but forgot to be. Loose fiberglass fiber is what I was refering to.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×