#21 Chilly

Chilly

    those who know, teach

  • Members
  • PipPipPip
  • 895 posts
  • LocationLangdon Hills, Essex, UK

Posted 16 February 2015 - 03:01 AM

The link had excess characters at the end, try http://beadglass.com.au/


----------------------------------------------------------

Ann

http://www.readypeda...uk/pottery.html


#22 NancyAmores

NancyAmores

    mostly beads & tile

  • Members
  • PipPipPip
  • 75 posts
  • LocationRhode Island

Posted 21 February 2015 - 03:22 PM

Wanted to add that Kanthal wire 16 gauge and up is on Amazon for pretty cheap. The wire is used in nicotine vaporizers. I've fired it to cone 6 with no problem, the description says it can go up to 2550F, so cone 10 should also be fine.