I share a studio with some friends in London. We recently acquired a secondhand electric kiln. We have a backlog of lots of stoneware to fire and a few terracotta pieces. Can we put them both in the kiln for bisque firing? Sorry to be so ignorant but we are beginners.

Share this post


Link to post
Share on other sites

I share a studio with some friends in London. We recently acquired a secondhand electric kiln. We have a backlog of lots of stoneware to fire and a few terracotta pieces. Can we put them both in the kiln for bisque firing? Sorry to be so ignorant but we are beginners.

 

 

Stoneware and earthenware can be fired together for the bisque firing i.e. at around 1,000 degrees centigrade.

Share this post


Link to post
Share on other sites

I share a studio with some friends in London. We recently acquired a secondhand electric kiln. We have a backlog of lots of stoneware to fire and a few terracotta pieces. Can we put them both in the kiln for bisque firing? Sorry to be so ignorant but we are beginners.

 

 

Stoneware and earthenware can be fired together for the bisque firing i.e. at around 1,000 degrees centigrade.

 

 

Thank you so much for that. I will try it tomorrow.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.