Two of my test glazes ran onto a kiln shelf. I swear the glazes ate partially through the shelf. I know I have to grind out all the glaze. This is leaving a gouge in the shelf. Is there something I can use to permanently fill that area before decorating with kiln wash?

Share this post


Link to post
Share on other sites

Two of my test glazes ran onto a kiln shelf. I swear the glazes ate partially through the shelf. I know I have to grind out all the glaze. This is leaving a gouge in the shelf. Is there something I can use to permanently fill that area before decorating with kiln wash?

 

 

You know I have the same problem...pitted kiln shelves...I'm thinking kiln cement might work but am anxious to hear what others think about this too.

Share this post


Link to post
Share on other sites

just wash right over it. if the shelf gets really bad after repeat cleanups, simply buy another shelf and keep the old one as a "waste shelf" that you don't mind messing up. standard kiln shelves are pretty cheap IMO when you compare it to the high-tech ones out now.

 

i always make students test glazes in a pre-fired firing tray or saggar simply to avoid this exact problem.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.