Any advice on how to control the expansion in this low fire white casting slip?

It is shivering off commercial glazes:

 

.400 TEXAS TALC

.250 C&C

.200 HYDRITE FLAT

.100 MINSPAR 200

.050 VICRON 25-11Any ideas much appreciated !

 

 

Share this post


Link to post
Share on other sites

.400 TEXAS TALC

.250 C&C

.200 HYDRITE FLAT

.100 MINSPAR 200

.050 VICRON 25-11Any ideas much appreciated !

Well for starters please give some more details on the materials like the C&C? what is that?

.400 Talc

.200 C&C what is this material?

.200 Hydrite flat this is EPK but an unusual brand used in paints I think

.100 Minspar-just a spar

.050 Vicron which is whiting or limestone take your pick

You said(It is shivering off commercial glazes)

do you mean low fire glazes are shivering off the clay or are you applying this over the glaze and it comes off?

Mark

Share this post


Link to post
Share on other sites

.400 TEXAS TALC

.250 C&C

.200 HYDRITE FLAT

.100 MINSPAR 200

.050 VICRON 25-11Any ideas much appreciated !

Well for starters please give some more details on the materials like the C&C? what is that?

.400 Talc

.200 C&C what is this material?

.200 Hydrite flat this is EPK but an unusual brand used in paints I think

.100 Minspar-just a spar

.050 Vicron which is whiting or limestone take your pick

You said(It is shivering off commercial glazes)

do you mean low fire glazes are shivering off the clay or are you applying this over the glaze and it comes off?

Mark

 

 

Thanks For taking a look at this Mark !

The commercial glazes are shivering off the cast pieces.

From Digital Fire: C+C = White burning plastic ball clay: Considered by some as a stoneware clay, it fires very white and is used in white firing porcelains and stoneware for its excellent plasticity.The company describes it as a fine-grained engineered blend, well known for its excellent plasticity and fired properties. This consistent blend is suitable for a wide variety of forming processes, where a high degree of plasticity is required, such as dry pressing, jiggering, ram pressing and casting.

 

Hydrite Imery's A coarse particle, acid flocculated kaolin clay with controlled particle distribution.

Share this post


Link to post
Share on other sites

I'd start with a real shrinkage test. Then we can go from there. 500C isn't even 1000F. You've gotta be fiirng hotter than that.

 

C&C is my favorite ball clay. It's wonderful stuff- more plastic and way more consistent than OM4. It's a blend of Champion and Challenger clays, from H.C. Spinks.

Share this post


Link to post
Share on other sites

I'd start with a real shrinkage test. Then we can go from there. 500C isn't even 1000F. You've gotta be fiirng hotter than that.

 

C&C is my favorite ball clay. It's wonderful stuff- more plastic and way more consistent than OM4. It's a blend of Champion and Challenger clays, from H.C. Spinks.

 

 

That test was done by Gare; not sure why sooo low temp: but maybe some relative info will be informative:

From the same test: Standard slip – 9.11 and Miller NS1 slip – 7.8.

 

I am seeing online that a lot of folks use 50% talc in low fare casting slip: maybe that is the ticket?

Share this post


Link to post
Share on other sites

Can you post pictures of "shivering". Please

 

 

off topic but I cant help but ask,

 

Why one would want to mix casting slip when it can be bought so cheaply and easily.

 

I have uses tons of laguna clay co. slip comes dry, 50 pound sacks, at about 25 cents a pound. So easy, its all in there

 

10 years using and always exactly the same, perfect glaze fit, etc

 

just cant imagine messing with ingredients and blending etc...

 

okay carry on,

 

good luck

big D

Share this post


Link to post
Share on other sites

Can you post pictures of "shivering". Please

 

 

off topic but I cant help but ask,

 

Why one would want to mix casting slip when it can be bought so cheaply and easily.

 

I have uses tons of laguna clay co. slip comes dry, 50 pound sacks, at about 25 cents a pound. So easy, its all in there

 

10 years using and always exactly the same, perfect glaze fit, etc

 

just cant imagine messing with ingredients and blending etc...

 

okay carry on,

 

good luck

big D

 

Hey BigD. I work at a place like laguna and we are vexed because this formula works for some and not others

I agree.. I would never make the stuff myself... nor will I ever make my own clay ! :)

Share this post


Link to post
Share on other sites

 

 

To get a slip that works better and looks better than any you can buy.

 

Jim

 

I suppose,

we did go through tons of supplies in school trying out recipes for casting slip, never came close to anything as good as the off the shelf stuff I use now

 

so that skews my view I guess.

 

carry on...

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.