Should outdoor pieces be glazed on the interior of the piece to prevent future problems?

I painted a bisque piece at a studio recently and they glazed and fired it. I noticed when I went to put the piece in my garden that the inside of the piece still had that chalky bisque feel to it. I didn't paint the inside. I thought they dip the whole piece in the glaze (inside and outside), not just the outside painted areas before they fire it. That way the inside would be smooth and shiny like the outside painted parts.

Is this a normal procedure for outdoor pieces? Won't this cause a problem with moisture getting inside the piece since the bottom of the piece has a big opening and will be sitting in the dirt?. It seems like it would eventually disinagrate or the paint would separate from the piece.

#2 Biglou13

Biglou13

    Advanced Member

  • Members
  • PipPipPip
  • 1,258 posts
  • LocationNorth Florida

Posted 21 April 2013 - 03:56 AM

A good start would be understanding vitrification.

Many people have pottery gardens, and these pieces both glazed and not.,and sitting in the dirt will out live many of our life times.

Glaze may make clay water resistant, but can also cause physical problems.

Much depends on sentence one.

There will be other along with more scholarly response.

LEC potttery  on facebook, instagram

 

The true sign of intelligence is not knowledge but imagination.
-Albert Einstein


#3 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,217 posts
  • LocationRed Lodge, Montana

Posted 21 April 2013 - 07:48 AM

Actually "spawling" can happen when moisture gets behind a glaze on a clay that is too porous and pop the glaze off.
It is best to use a freeze resistant clay. There are terra cotta recipes for this.

Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#4 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,092 posts
  • LocationRaleigh, NC

Posted 21 April 2013 - 10:58 AM

I have a lot of work in my yard ... Glazed only on outer surfaces or not glazed at all. This is in North Carolina where it does freeze, but not for months on end. Some have been out there for 18 - 20 years with no obvious damage. The ones that lasted the shortest time were the raku pieces. Glazed or unglazed they have fallen apart ... I guess because they were softer??
Chris Campbell Pottery
Contemporary Fine Colored Porcelain
http://ccpottery.com/

>TRY ... FAIL ... LEARN ... REPEAT"

" If a sufficient number of people are different, no one has to be normal "

Fredrick Bachman




0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users