Hi - I am making my first coil pot - a bowl or maybe a vase - (I am new to this) and wanted to put a decorative crack penetrating the entire thickness (preferably just one if that is possible).
I saw a youtube video of someone using a small hammer after it had been fired(?). The sides looked thin (maybe done on a wheel?) and she made a bigger crack than I would want to do. Should I think of switching to slab to control thickness? Would it be possible to cut the vase in 2 pieces and either intentionally put them back together unevenly before firing, or firing the 2 pieces and then gluing them back together unevenly?
It would be a decorative piece and doesn't need to hold water. As you can see I know nothing about this so any info would be helpful! Thanks-

PS- Here is a pic of the feeling I want for the pot, but maybe just one crack going up the bowl or vase.

#2 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,136 posts
  • LocationRed Lodge, Montana

Posted 21 April 2013 - 07:46 AM

Hi - I am making my first coil pot - a bowl or maybe a vase - (I am new to this) and wanted to put a decorative crack penetrating the entire thickness (preferably just one if that is possible).
I saw a youtube video of someone using a small hammer after it had been fired(?). The sides looked thin (maybe done on a wheel?) and she made a bigger crack than I would want to do. Should I think of switching to slab to control thickness? Would it be possible to cut the vase in 2 pieces and either intentionally put them back together unevenly before firing, or firing the 2 pieces and then gluing them back together unevenly?
It would be a decorative piece and doesn't need to hold water. As you can see I know nothing about this so any info would be helpful! Thanks-

PS- Here is a pic of the feeling I want for the pot, but maybe just one crack going up the bowl or vase.


I didn't see a link to a picture. Are you familiar with Stephen Lee's work?
Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#3 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,066 posts
  • LocationRaleigh, NC

Posted 21 April 2013 - 11:03 AM

No image seen but to answer your question, yes you could build one pot ... Wait til it is cheese hard ... Cut if up / crack it ... any way you want and re-assemble it using slip made from the same clay.

Chris Campbell

Contemporary Fine Colored Porcelain
www.ccpottery.com

 

TRY ... FAIL ... LEARN ... REPEAT

" ... If a sufficient number of people are different, no one has to be normal"
Fredrick Bachman


#4 Cathy Linfield

Cathy Linfield

    Newbie

  • Members
  • Pip
  • 1 posts

Posted 21 April 2013 - 11:19 AM

Hi - I am making my first coil pot - a bowl or maybe a vase - (I am new to this) and wanted to put a decorative crack penetrating the entire thickness (preferably just one if that is possible).
I saw a youtube video of someone using a small hammer after it had been fired(?). The sides looked thin (maybe done on a wheel?) and she made a bigger crack than I would want to do. Should I think of switching to slab to control thickness? Would it be possible to cut the vase in 2 pieces and either intentionally put them back together unevenly before firing, or firing the 2 pieces and then gluing them back together unevenly?
It would be a decorative piece and doesn't need to hold water. As you can see I know nothing about this so any info would be helpful! Thanks-

PS- Here is a pic of the feeling I want for the pot, but maybe just one crack going up the bowl or vase.


You might try slicing almost all the way through the pot when it is almost leather hard, let it dry further then slice all the way through. Make sure you low fire for a couple hours...OR.... put it in your oven and take it from 100F to 350F in 3 hours....Slow drying will help it to not crack further . Cathy

#5 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,136 posts
  • LocationRed Lodge, Montana

Posted 21 April 2013 - 12:13 PM

Stephen Lee is the Director at the ARchie Bray and recently open a show in NYC. Some pieces were from this series
http://www.ferringal...nt_8303_374.jpg

Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#6 Chris Throws Pots

Chris Throws Pots

    Advanced Member

  • Members
  • PipPipPip
  • 97 posts
  • LocationVermont

Posted 21 April 2013 - 12:57 PM

Check out Jeff Campana's work. http://jeffcampana.com/

Christopher Vaughn Pottery
Functional stoneware forms
handcrafted in Burlington, Vermont

 

www.ChrisThrowsPots.com

 

On Instagram @chris_throws_pots
 

 

 

 


#7 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,066 posts
  • LocationRaleigh, NC

Posted 21 April 2013 - 03:15 PM

Check out Jeff Campana's work. http://jeffcampana.com/


Thanks for this link ... Terrific work and a most interesting process.

Chris Campbell

Contemporary Fine Colored Porcelain
www.ccpottery.com

 

TRY ... FAIL ... LEARN ... REPEAT

" ... If a sufficient number of people are different, no one has to be normal"
Fredrick Bachman


#8 kgtys

kgtys

    Member

  • Members
  • PipPip
  • 11 posts

Posted 21 April 2013 - 06:12 PM

Posted Today, 10:25 PM

Hi - I am making my first coil pot - a bowl or maybe a vase - (I am new to this) and wanted to put a decorative crack penetrating the entire thickness (preferably just one if that is possible).
I saw a youtube video of someone using a small hammer after it had been fired(?). The sides looked thin (maybe done on a wheel?) and she made a bigger crack than I would want to do. Should I think of switching to slab to control thickness? Would it be possible to cut the vase in 2 pieces and either intentionally put them back together unevenly before firing, or firing the 2 pieces and then gluing them back together unevenly?
It would be a decorative piece and doesn't need to hold water. As you can see I know nothing about this so any info would be helpful! Thanks-

PS- Here is a pic of the feeling I want for the pot, but maybe just one crack going up the bowl or vase.


#9 kgtys

kgtys

    Member

  • Members
  • PipPip
  • 11 posts

Posted 21 April 2013 - 06:27 PM


Hi - I am making my first coil pot - a bowl or maybe a vase - (I am new to this) and wanted to put a decorative crack penetrating the entire thickness (preferably just one if that is possible).
I saw a youtube video of someone using a small hammer after it had been fired(?). The sides looked thin (maybe done on a wheel?) and she made a bigger crack than I would want to do. Should I think of switching to slab to control thickness? Would it be possible to cut the vase in 2 pieces and either intentionally put them back together unevenly before firing, or firing the 2 pieces and then gluing them back together unevenly?
It would be a decorative piece and doesn't need to hold water. As you can see I know nothing about this so any info would be helpful! Thanks-

PS- Here is a pic of the feeling I want for the pot, but maybe just one crack going up the bowl or vase.


You might try slicing almost all the way through the pot when it is almost leather hard, let it dry further then slice all the way through. Make sure you low fire for a couple hours...OR.... put it in your oven and take it from 100F to 350F in 3 hours....Slow drying will help it to not crack further . Cathy



#10 kgtys

kgtys

    Member

  • Members
  • PipPip
  • 11 posts

Posted 21 April 2013 - 06:29 PM

Posted Today, 10:25 PM

Hi - I am making my first coil pot - a bowl or maybe a vase - (I am new to this) and wanted to put a decorative crack penetrating the entire thickness (preferably just one if that is possible).
I saw a youtube video of someone using a small hammer after it had been fired(?). The sides looked thin (maybe done on a wheel?) and she made a bigger crack than I would want to do. Should I think of switching to slab to control thickness? Would it be possible to cut the vase in 2 pieces and either intentionally put them back together unevenly before firing, or firing the 2 pieces and then gluing them back together unevenly?
It would be a decorative piece and doesn't need to hold water. As you can see I know nothing about this so any info would be helpful! Thanks-

PS- Here is a pic of the feeling I want for the pot, but maybe just one crack going up the bowl or vase.



#11 kgtys

kgtys

    Member

  • Members
  • PipPip
  • 11 posts

Posted 21 April 2013 - 06:35 PM

Thanks Cathy - that sounds manageble for me!


Hi - I am making my first coil pot - a bowl or maybe a vase - (I am new to this) and wanted to put a decorative crack penetrating the entire thickness (preferably just one if that is possible).
I saw a youtube video of someone using a small hammer after it had been fired(?). The sides looked thin (maybe done on a wheel?) and she made a bigger crack than I would want to do. Should I think of switching to slab to control thickness? Would it be possible to cut the vase in 2 pieces and either intentionally put them back together unevenly before firing, or firing the 2 pieces and then gluing them back together unevenly?
It would be a decorative piece and doesn't need to hold water. As you can see I know nothing about this so any info would be helpful! Thanks-

PS- Here is a pic of the feeling I want for the pot, but maybe just one crack going up the bowl or vase.
[/quote]

You might try slicing almost all the way through the pot when it is almost leather hard, let it dry further then slice all the way through. Make sure you low fire for a couple hours...OR.... put it in your oven and take it from 100F to 350F in 3 hours....Slow drying will help it to not crack further . Cathy
[/quote]
[/quote]

#12 kgtys

kgtys

    Member

  • Members
  • PipPip
  • 11 posts

Posted 21 April 2013 - 06:38 PM

[quote name='Chris Campbell' date='21 April 2013 - 01:15 PM' timestamp='1366575332' post='33348']
[quote name='Chris Throws Pots' date='21 April 2013 - 01:57 PM' timestamp='1366567063' post='33344']
Check out Jeff Campana's work. http://jeffcampana.com/
[/quote]

Thanks for this link ... Terrific work and a most interesting process.

Thanks Chris - beautiful stuff!

#13 kgtys

kgtys

    Member

  • Members
  • PipPip
  • 11 posts

Posted 21 April 2013 - 06:43 PM

[quote name='kgtys' date='21 April 2013 - 04:35 PM' timestamp='1366587325' post='33358']
Thanks Cathy - that sounds manageble for me!


Hi - I am making my first coil pot - a bowl or maybe a vase - (I am new to this) and wanted to put a decorative crack penetrating the entire thickness (preferably just one if that is possible).
I saw a youtube video of someone using a small hammer after it had been fired(?). The sides looked thin (maybe done on a wheel?) and she made a bigger crack than I would want to do. Should I think of switching to slab to control thickness? Would it be possible to cut the vase in 2 pieces and either intentionally put them back together unevenly before firing, or firing the 2 pieces and then gluing them back together unevenly?
It would be a decorative piece and doesn't need to hold water. As you can see I know nothing about this so any info would be helpful! Thanks-

PS- Here is a pic of the feeling I want for the pot, but maybe just one crack going up the bowl or vase.
[/quote]

You might try slicing almost all the way through the pot when it is almost leather hard, let it dry further then slice all the way through. Make sure you low fire for a couple hours...OR.... put it in your oven and take it from 100F to 350F in 3 hours....Slow drying will help it to not crack further . Cathy
[/quote]
[/quote]
[/quote]

Thanks Cathy - That sounds manageble for me!


#14 kgtys

kgtys

    Member

  • Members
  • PipPip
  • 11 posts

Posted 21 April 2013 - 06:48 PM

Stephen Lee is the Director at the ARchie Bray and recently open a show in NYC. Some pieces were from this series
http://www.ferringal...nt_8303_374.jpg

Marcia


Thanks Marcia I learn alot form these great visuals!




0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users