Posted 18 April 2013 - 02:16 PM

Can I use low fire glazes on cone 6 clay? What would happen?

#2 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 4,826 posts
  • LocationGrayslake, IL

Posted 18 April 2013 - 02:31 PM

The glazes will likely craze. Bad glaze fit.

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

[email protected]


#3 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,067 posts
  • LocationRaleigh, NC

Posted 18 April 2013 - 02:48 PM

Neil is right ... You will either under fire the clay or over fire the glaze.
Under fired clay is weak and over fired glazes crack and/or run.

However ... It all depends on what you want to do and how you want to do it.
If you love the glaze color and can't get it any other way then you have to adapt.
You could fire the clay to its temperature of Cone 6 then glaze it and re fire to Cone 04-06
If it were a sculpture or other non functional object you could just glaze and fire the whole thing cooler ... Maybe not as low as Cone 04 ... you might try higher temps to see what happens. Maybe Cone 2, 3 or 4? Put it on something so if it runs you won't have a shelf to clean.

Chris Campbell

Contemporary Fine Colored Porcelain
www.ccpottery.com

 

TRY ... FAIL ... LEARN ... REPEAT

" ... If a sufficient number of people are different, no one has to be normal"
Fredrick Bachman


#4 Iforgot

Iforgot

    Advanced Member

  • Members
  • PipPipPip
  • 155 posts
  • LocationColorado

Posted 18 April 2013 - 08:35 PM

Neil is right ... You will either under fire the clay or over fire the glaze.
Under fired clay is weak and over fired glazes crack and/or run.

However ... It all depends on what you want to do and how you want to do it.
If you love the glaze color and can't get it any other way then you have to adapt.
You could fire the clay to its temperature of Cone 6 then glaze it and re fire to Cone 04-06
If it were a sculpture or other non functional object you could just glaze and fire the whole thing cooler ... Maybe not as low as Cone 04 ... you might try higher temps to see what happens. Maybe Cone 2, 3 or 4? Put it on something so if it runs you won't have a shelf to clean.



Smart, Smart
Derek VonDrehle

Raku, Pit fired, Majolica, and Stoneware ceramic artisit

#5 oldlady

oldlady

    single firing an electric kiln to cone 6

  • Members
  • PipPipPip
  • 3,234 posts
  • Locationharpers ferry west va and pinellas park fl

Posted 02 May 2013 - 11:54 PM

gypsy, your title suggests that you might think that cone 06 is hotter than cone 04. the reverse is true. maybe i am misreading you or maybe i have always assumed that whenever anyone talks about a range of temperatures the lower number is mentioned first. from low to high.
"putting you down does not raise me up."

#6 Nat

Nat

    Member

  • Members
  • PipPip
  • 15 posts

Posted 03 May 2013 - 12:03 PM

I often use earthenware glazes on a stoneware body...sometimes it crazes, sometimes not...I happen to love the crackle effect though, but if you're glazing items that need to be food safe, it's not so good.

#7 Claypple

Claypple

    Advanced Member

  • Members
  • PipPipPip
  • 261 posts
  • LocationReno, NV

Posted 03 May 2013 - 07:06 PM

The answer depends on what Gypsy is making and what glaze she is using.

Chris is right, re-firing up to ^6 and then glazing at ^06 probably is the most common solution.

#8 gypsy

gypsy

    Advanced Member

  • Members
  • PipPipPip
  • 89 posts
  • LocationJames Creek, Pa

Posted 03 May 2013 - 08:41 PM

Thanks everyone. I have cone 6 clay and wanted to fire mayco specialty glazes but didnt know if it would work.

#9 ashleigh_arts

ashleigh_arts

    Member

  • Members
  • PipPip
  • 23 posts
  • LocationArkansas

Posted 20 February 2014 - 09:00 PM

Did you try this, Gypsy? What were your results? I'm curious, also!