Hello,

I'm not sure if this forum is a good place to ask this or not. I was in Japan and bought this ceramic pot (actually a foot-warmer), it is about the size of a wok and has a lid. Anyway I dropped it on the way back, in it's box, and there is a crack going all the way down the side now. Is this thing repairable? I was thinking there may be some kind of fireproof ceramic glue that would work -- but maybe not. Anyone with ceramics experience know?

Thanks for any suggestions,
Bob

#2 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,069 posts
  • LocationRaleigh, NC

Posted 15 April 2013 - 03:38 PM

Can you attach a picture? We might be able to give you better advice if we can see it.

Chris Campbell

Contemporary Fine Colored Porcelain
www.ccpottery.com

 

TRY ... FAIL ... LEARN ... REPEAT

" ... If a sufficient number of people are different, no one has to be normal"
Fredrick Bachman


#3 perkolator

perkolator

    Advanced Member

  • Members
  • PipPipPip
  • 428 posts
  • LocationCalifornia

Posted 15 April 2013 - 06:20 PM

sorry, but i would personally say no, there is no repair for this piece...sounds like you have a nice-size structural crack in the vessel if it goes all the way down the side. even with re-firing the piece I doubt anyone could make a repair strong enough to warrant it being "safe" to use as intended. glue it back together and just admire it.

#4 bsabiston

bsabiston

    Newbie

  • Members
  • Pip
  • 2 posts

Posted 16 April 2013 - 08:50 AM

Can you attach a picture? We might be able to give you better advice if we can see it.


Here are some pictures.

Attached Files



#5 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 4,828 posts
  • LocationGrayslake, IL

Posted 16 April 2013 - 09:22 AM

There is no firing method that can repair it back to new. The best you can do is epoxy it back together it, but it will not be functional.

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

[email protected]


#6 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,069 posts
  • LocationRaleigh, NC

Posted 16 April 2013 - 09:49 AM

I agree ... you now have a lovely conversation piece. I would not even put water in it when repaired.
It is lovely though!

Chris Campbell

Contemporary Fine Colored Porcelain
www.ccpottery.com

 

TRY ... FAIL ... LEARN ... REPEAT

" ... If a sufficient number of people are different, no one has to be normal"
Fredrick Bachman





0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users