Posted 12 April 2013 - 04:24 PM

I have about 10 Mother's Day mugs I made with kids. I got them to decorate with coloured slips while leather hard. Now I am looking for a shiny cone 06 clear that will work with reds and purples. This is not my temperature, other than using commercial glazes. I just want to dip these and fire them in my bisque kiln.
Thanks,TJR.

#2 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 4,904 posts
  • LocationGrayslake, IL

Posted 13 April 2013 - 08:16 AM

90% Ferro Frit 3124
10% EPK

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

neil@neilestrickgallery.com


#3 TJR

TJR

    Advanced Member

  • Members
  • PipPipPip
  • 1,821 posts
  • LocationWinnipeg,Manitoba,Canada

Posted 13 April 2013 - 10:04 AM

90% Ferro Frit 3124
10% EPK


Neil;
Thanks, buddy.I only need 1000 grams, so will mix up an ice cream pail.