Jump to content


Photo
- - - - -

Propane Burners


  • Please log in to reply
12 replies to this topic

#1 Glen Peters

Glen Peters

    Advanced Member

  • Members
  • PipPipPip
  • 47 posts

Posted 12 April 2013 - 08:42 AM

I bought a propane burner and wondered whether it would be appropriate for a small raku kiln (modified 45Gal drum)

This burner is rated at 500,000 BTU/Hr. It was on sale for for $60.00 Cnd regular $80.00 And if 500,000 isn't enough I could buy two???

(check link)
My link

#2 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 5,051 posts
  • LocationGrayslake, IL

Posted 12 April 2013 - 10:28 AM

More than large enough. Have fun!

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

[email protected]


#3 TJR

TJR

    Advanced Member

  • Members
  • PipPipPip
  • 1,821 posts
  • LocationWinnipeg,Manitoba,Canada

Posted 12 April 2013 - 11:47 AM

Glen;
You probably want to get a regulator as well from your propane supplier. Looks like a gauge about 2 inches in diameter. Screws into your tank, then the hose comes from that. Might be reverse threaded so go easy with the wrench. I agree with Neil. Have fun.
TJR.Posted Image

#4 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,359 posts
  • LocationRed Lodge, Montana

Posted 12 April 2013 - 11:57 AM

It's a go! Have fun. I set my regulators at 3.5 lbs. I fire with 2 burners but I have a large raku kiln. It is in my gallery.
I am having perfect weather for Raku at the moment.
Marcia


Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#5 Glen Peters

Glen Peters

    Advanced Member

  • Members
  • PipPipPip
  • 47 posts

Posted 12 April 2013 - 02:31 PM

Thank you all

That burner is two inches. And I assume your saying that "one" burner should more than enough?

Glen

#6 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 5,051 posts
  • LocationGrayslake, IL

Posted 12 April 2013 - 03:08 PM

Yes, that one is more than enough.

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

[email protected]


#7 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,359 posts
  • LocationRed Lodge, Montana

Posted 12 April 2013 - 04:47 PM

500,000 BTUs is plenty. What size is your kiln and what materials? That is the only thing that would make a difference. If you have a huge raku kiln made out of straw (joking) or poor insulation material
Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#8 jrgpots

jrgpots

    The hands can express the soul

  • Members
  • PipPipPip
  • 806 posts
  • LocationHurricane, Utah

Posted 12 April 2013 - 05:25 PM

It's a go! Have fun. I set my regulators at 3.5 lbs. I fire with 2 burners but I have a large raku kiln. It is in my gallery.
I am having perfect weather for Raku at the moment.
Marcia




Make sure the regulater is a high pressure regulator( usually 1 to 10 lbs pressure) not the type for a BBQ or fireplace.

#9 Glen Peters

Glen Peters

    Advanced Member

  • Members
  • PipPipPip
  • 47 posts

Posted 13 April 2013 - 06:57 AM


It's a go! Have fun. I set my regulators at 3.5 lbs. I fire with 2 burners but I have a large raku kiln. It is in my gallery.
I am having perfect weather for Raku at the moment.
Marcia

Marcia, I havent built one yet but I was kinda thinking a 45 gallon drum lined with fiber?




Make sure the regulater is a high pressure regulator( usually 1 to 10 lbs pressure) not the type for a BBQ or fireplace.


Ok Thanks!

#10 Glen Peters

Glen Peters

    Advanced Member

  • Members
  • PipPipPip
  • 47 posts

Posted 17 April 2013 - 03:17 PM

It's a go! Have fun. I set my regulators at 3.5 lbs. I fire with 2 burners but I have a large raku kiln. It is in my gallery.
I am having perfect weather for Raku at the moment.
Marcia

Hi Marcia

I'm having trouble sourcing a high pressure propane regulator... any ideas where I might find one? Yours has a gauge I assume?

Thanks



#11 Glen Peters

Glen Peters

    Advanced Member

  • Members
  • PipPipPip
  • 47 posts

Posted 18 April 2013 - 12:16 PM

Hi all

Regarding my burner question, I have been looking at regulators and wondered if I needed a gauge with it? This reg doesn't have a gauge but claims to be ajustable from 0 to 30, will it do the trick?
My link

Thanks
Glen

#12 Brian Reed

Brian Reed

    Advanced Member

  • Members
  • PipPipPip
  • 219 posts
  • LocationWashington State

Posted 19 April 2013 - 06:09 PM

I would not get one without a gauge. I would look for one more like this example, but in lower pressure. Although this does state 0-70 psi I would be leary of one that had such a large range so fine .5 and .25 PSI adjustments may be hard.



My link
Brian Reed

Throwing down in Washington State

http://www.reedpottery.com

Northwest Clay Club

#13 Glen Peters

Glen Peters

    Advanced Member

  • Members
  • PipPipPip
  • 47 posts

Posted 19 April 2013 - 09:09 PM

I would not get one without a gauge. I would look for one more like this example, but in lower pressure. Although this does state 0-70 psi I would be leary of one that had such a large range so fine .5 and .25 PSI adjustments may be hard.

Thanks Brian I'm glad I asked!



My link