I've been altering manufactured to clay to get away from the out of the box look, and it ads ownership to my medium/art, with much success. I' ve heard/ read where sawdust is wedged into clay.

 

What does this do? Technically speaking.

How does it change look or feel?

How will it afflect glaze? ( will run tests)

How much sawdust is good staring point?

I'm planning on using dust from sander so it's pretty fine.

How would coarse sawdust vs fine sawdust differ?

It will be fired cone 6 electric ox, (pending studio owner approval) however I first head of this with wood fired.

 

Thanks in advance for any advice, comments, answers.

Share this post


Link to post
Share on other sites

only time I have used saw dust into a clay body was when I was making water filters ... but that was to create a clay that had pockets in the body. We had a guest at my university from potters with peace that would teach places with unclean water to make them from local clays. Awesome stuff too. Ended up making some for some people who had hunting cabins out in the boonies of florida when I still lived in that part of the world.

 

 

 

 

Really though, any sort of material like saw dust most likely won't show up in the final product as it burns out and can probably make the product weaker since you have holes in the middle of the clay body. ... now embedded into the surface will create a rough texture depending on how fine the dust is ... otherwise you won't see many effects since burnout won't really trap ash so it won't affect glazing in that aspect and only surface burnout will affect the glaze by pooling so the finer the burnout ... the less you will likely see it.

Share this post


Link to post
Share on other sites

I tried using sawdust, for some pit fired pieces, as I read that it could reduce the risk for thermal shock. It didn't seem to help, but there were other factors, that contributed to the issue.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×