Do electronic kiln controlers actually simulate heat work on pyrometric cones or do they just measure air temperature?

Joel.

#2 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 5,050 posts
  • LocationGrayslake, IL

Posted 04 April 2013 - 11:21 AM

Controllers take into account rate of climb, etc, to simulate heat work.

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

[email protected]


#3 JBaymore

JBaymore

    Moderator

  • Moderators
  • 4,267 posts
  • LocationWilton, NH USA

Posted 04 April 2013 - 11:56 AM

And the panel at NCECA that included significant players in the filed of controllers talked about how relatively primitive the cone behavior model is that is used in those various controllers at this time.

So let the controller function to guide the ramping and holds aspects of the firing, but use witness cones as the "final say" on your claywork until the next generation of these things is available.

best,


..................john

John Baymore
Adjunct Professor of Ceramics; New Hampshire Insitute of Art

Former Guest Professor, Wuxi Institute of Arts and Science, Yixing, China

Former President and Past President; Potters Council
 

http://www.JohnBaymore.com

http://www.nhia.edu/...ty/john-baymore


#4 yedrow

yedrow

    Advanced Member

  • Members
  • PipPipPip
  • 405 posts

Posted 04 April 2013 - 02:55 PM

Thanks guys!!! It is very kind of you both to be so generous with your expertise.

Joel.

#5 jrgpots

jrgpots

    The hands can express the soul

  • Members
  • PipPipPip
  • 805 posts
  • LocationHurricane, Utah

Posted 10 April 2013 - 09:48 PM

If I were to buy a controller, should I get a single zone vs multiple zone controller? How many segments? And should I get it with or without a KISS interface?:mellow:src="http://ceramicartsda...lt/mellow.gif">

#6 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 5,050 posts
  • LocationGrayslake, IL

Posted 11 April 2013 - 02:56 PM

If I were to buy a controller, should I get a single zone vs multiple zone controller? How many segments? And should I get it with or without a KISS interface?:mellow:src="http://ceramicartsda...lt/mellow.gif">


Multi zone is awesome. Much more consistent firings than single zone, and firings are not really affected by how you load the kiln.


The KISS interface is a toy, in my opinion. It lets you look at all sorts of numbers pertaining to the firing, which is interesting, but kilns are not all that accurate in engineering terms, so all that really detailed information doesn't really help you out that much. Maybe if you're doing some super touchy crystalline type work, but that's it. I've had customers who demanded I fix their kilns because the KISS software showed some inconsistencies in the firings, even though the pots all looked the same, and looked like they were supposed to. They got so hung up on numbers that they couldn't see that the pots were fine.

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

[email protected]


#7 jrgpots

jrgpots

    The hands can express the soul

  • Members
  • PipPipPip
  • 805 posts
  • LocationHurricane, Utah

Posted 11 April 2013 - 06:09 PM

Thanks for the useful info....Saving my pennies for a Bartlett multi zone controller....


Jed




0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users