Posted 01 April 2013 - 04:11 PM

We have a very large pot that we use for an outdoor water feature. This past winter we had a few abnormal freezes for Phoenix AZ and the glaze on the pot has started to pop and crack revealing the red clay.
The pot is only a couple years old and was expensive. The fountain has been turned off, the pot removed and dryed. Is there product to use or something we can do keep the rest of the glaze from cracking/popping off?
Any help you could give, would be greatly appreciated. (photo of area is attached) Thank you.

#2 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,117 posts
  • LocationRaleigh, NC

Posted 01 April 2013 - 07:39 PM

Sorry, no photo showing here ... could you try attaching the photo again?
Chris Campbell Pottery
Contemporary Fine Colored Porcelain
http://ccpottery.com/

>TRY ... FAIL ... LEARN ... REPEAT"

" If a sufficient number of people are different, no one has to be normal "

Fredrick Bachman




0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users