using two company glazes...toxic ?

Recommended Posts

bciskepottery    925

Any time you overlap two different glazes . . . you create a new, third glaze. And, depending on the contents of the two glazes, you could end up with an unstable/nondurgable glaze that leeches a coloring oxide, etc. Doesn't matter if the glazes were made by two different companies or the same company. Putting a "safe" clear over a "problem" glaze will not automatically make the resulting glaze safe . . . you need to test it.

Share this post


Link to post
Share on other sites
Fish Lady    0

Any time you overlap two different glazes . . . you create a new, third glaze. And, depending on the contents of the two glazes, you could end up with an unstable/nondurgable glaze that leeches a coloring oxide, etc. Doesn't matter if the glazes were made by two different companies or the same company. Putting a "safe" clear over a "problem" glaze will not automatically make the resulting glaze safe . . . you need to test it.

 

 

 

How do I test to see if it has become toxic?

Share this post


Link to post
Share on other sites
bciskepottery    925

Any time you overlap two different glazes . . . you create a new, third glaze. And, depending on the contents of the two glazes, you could end up with an unstable/nondurgable glaze that leeches a coloring oxide, etc. Doesn't matter if the glazes were made by two different companies or the same company. Putting a "safe" clear over a "problem" glaze will not automatically make the resulting glaze safe . . . you need to test it.

 

 

 

How do I test to see if it has become toxic?

 

 

 

Here's a start: http://digitalfire.com/4sight/education/are_your_glazes_food_safe_or_are_they_leachable_12.html

 

Also, consider picking up a copy of John Hesselberth/Ron Roy's "Mastering Cone 6 Glazes". The bible for making durable, stable glazes and how to test them at home.

Share this post


Link to post
Share on other sites
Fish Lady    0

Any time you overlap two different glazes . . . you create a new, third glaze. And, depending on the contents of the two glazes, you could end up with an unstable/nondurgable glaze that leeches a coloring oxide, etc. Doesn't matter if the glazes were made by two different companies or the same company. Putting a "safe" clear over a "problem" glaze will not automatically make the resulting glaze safe . . . you need to test it.

 

 

 

How do I test to see if it has become toxic?

 

 

 

Here's a start: http://digitalfire.c...achable_12.html

 

Also, consider picking up a copy of John Hesselberth/Ron Roy's "Mastering Cone 6 Glazes". The bible for making durable, stable glazes and how to test them at home.

 

 

 

Thank you... I currently have one dish with a lemon and another with vinegar.

Share this post


Link to post
Share on other sites
JBaymore    1,432
Thank you... I currently have one dish with a lemon and another with vinegar.

 

 

Note that those are only "rule in" tests not "rule out".

 

If they fail that test, you have no need to run a lab test. If they PASS that test, it does NOT say that it will not leach components. Only a standard acetic acid leach test will do that. (lab testing)

 

Note that if the glaze does not contain any toxics, then there is no need to test. It might be "bad" glass...... and deteriorate in visual character over time and use..... but it will not harm anyone.

 

best,

 

.......................john

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×