Posted 27 March 2013 - 06:58 PM

I've been looking for cone 5 recipes to start making my own glazes. I've been firing to cone 5 (oxidation) using commercial brush glazes. I want to start dipping. It seems that there are many cone 6 recipes, but not cone 5. Do I need to just start firing to cone 6, or can I use cone 6 glazes and just fire to cone 5? Also, I accidentally just posted a slip question on the "in the studio" forum vs the "glaze" forum. Also a recipe question... Thanks!

#2 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,069 posts
  • LocationRaleigh, NC

Posted 27 March 2013 - 07:13 PM

Your Cone 6 glazes will be under fired at Cone 5.
You need to fire glazes at the temperatures they are designed for or put up with them not looking right. : > )

Chris Campbell

Contemporary Fine Colored Porcelain
www.ccpottery.com

 

TRY ... FAIL ... LEARN ... REPEAT

" ... If a sufficient number of people are different, no one has to be normal"
Fredrick Bachman


#3 OffCenter

OffCenter

    Advanced Member

  • Members
  • PipPipPip
  • 1,372 posts

Posted 27 March 2013 - 07:22 PM

I've been looking for cone 5 recipes to start making my own glazes. I've been firing to cone 5 (oxidation) using commercial brush glazes. I want to start dipping. It seems that there are many cone 6 recipes, but not cone 5. Do I need to just start firing to cone 6, or can I use cone 6 glazes and just fire to cone 5? Also, I accidentally just posted a slip question on the "in the studio" forum vs the "glaze" forum. Also a recipe question... Thanks!


Consider firing to cone 6 instead of 5. The difference is so little that most cone 5 glazes look fine or maybe even better fired to cone 6. Usually, glazes look better over fired than under fired. Obviously, there is a chance that even that little over firing may make a glaze run so take precautions for that. Like most things in ceramics, the only way to find out is to test.

Jim
E pur si muove.

"But it does move," said Galileo under his breath.

#4 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,144 posts
  • LocationRed Lodge, Montana

Posted 28 March 2013 - 06:21 AM

I agree with Chris and Jim. You need to fire the glaze to the correct temperature. I have recipes posted in my gallery with pictures.
There are many good ^6 recipes out there. Firing schedules are critical for success. Read about soaking and down firing.

Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#5 John255

John255

    Advanced Member

  • Members
  • PipPipPip
  • 92 posts
  • LocationFlorida USA

Posted 28 March 2013 - 03:16 PM

I've been looking for cone 5 recipes to start making my own glazes. I've been firing to cone 5 (oxidation) using commercial brush glazes. I want to start dipping. It seems that there are many cone 6 recipes, but not cone 5. Do I need to just start firing to cone 6, or can I use cone 6 glazes and just fire to cone 5? Also, I accidentally just posted a slip question on the "in the studio" forum vs the "glaze" forum. Also a recipe question... Thanks!


Marge,
There can be a significant difference in the melt and surface appearance when firing a cone 5 glaze it to cone 6.
First the temperature between Orton large cone numbers is not linear.
There is a 65deg difference between large cone 5 and 6.
This has caused Orton to develop and now supply cone 5-1/2.
If you are firing with a kiln sitter you will find a difference between the sitter cone and the witness cone on the shelf.

The rate of firing also makes a significant difference in cone bending temperature.
The clay body the glaze is applied to will make the most visible difference.
Most of these details are never mentioned with glaze formulas.
You can find a lot of good firing info on the Orton website.
http://www.ortoncera...art_degreeF.pdf
Good luck,