      Ceramic Arts Network is looking for two new forum moderators for the Clay and Glaze Chemistry and Equipment Use and Repair sections of the Ceramic Arts Network Community Forum. We are looking for somebody who is an active participant (i.e. somebody who participates on a daily basis, or near daily) on the forum. Moderators must be willing to monitor the forum on a daily basis to remove spam, make sure members are adhering to the Forum Terms of Use, and make sure posts are in the appropriate categories. In addition to moderating their primary sections, Moderators must work as a team with other moderators to monitor the areas of the forum that do not have dedicated moderators (Educational Approaches and Resources, Aesthetic Approaches and Philosophy, etc.). Moderators must have a solid understanding of the area of the forum they are going to moderate (i.e. the Clay and Glaze Chemistry moderator must be somebody who mixes, tests, and has a decent understanding of materials). Moderators must be diplomatic communicators, be receptive to others’ ideas, and be able to see things from multiple perspectives. This is a volunteer position that comes with an honorary annual ICAN Gold membership. If you are interested, please send an email outlining your experience and qualifications to jharnetty@ceramics.org.
Sign in to follow this  
badmintonsyd

Paper Clay Ratios

Recommended Posts

I've been using my own porcelain paper clay recipe for the past year or so. I love how it looks once it's fired, but I'm having issues working with it wet sometimes. I have a feeling it might be the ratio for paper to clay that I've been using (I think I'm working with 30-40% paper). Anyone have any advice for me? Should I try another kind of fiber? ( For the paper, I just use single-ply toilet paper)

Share this post


Link to post
Share on other sites

I've been using my own porcelain paper clay recipe for the past year or so. I love how it looks once it's fired, but I'm having issues working with it wet sometimes. I have a feeling it might be the ratio for paper to clay that I've been using (I think I'm working with 30-40% paper). Anyone have any advice for me? Should I try another kind of fiber? ( For the paper, I just use single-ply toilet paper)

 

 

That seems like a high % of paper. My understanding is a maximum of 25%. Use anywhere from 15-25%

Marcia

Share this post


Link to post
Share on other sites

How are you guys measuring the paper, and is it wet clay by weight? I have only used paper clay for joining slip and then just threw a few sheets of toilet paper in a blender made a slurry, and then added bits of wet clay until it 'looked right'.

 

Is there a more accurate way to figure the ratio. Can't imaging weighing toilet paper, may be too early in the AM for me to grasp this, need more coffee.

Share this post


Link to post
Share on other sites

How are you guys measuring the paper, and is it wet clay by weight? I have only used paper clay for joining slip and then just threw a few sheets of toilet paper in a blender made a slurry, and then added bits of wet clay until it 'looked right'.

 

Is there a more accurate way to figure the ratio. Can't imaging weighing toilet paper, may be too early in the AM for me to grasp this, need more coffee.

 

 

 

How I did it was I made a paper slurry, then dried it so I had paper "pellets" and then measured from there

Share this post


Link to post
Share on other sites

I've been using my own porcelain paper clay recipe for the past year or so. I love how it looks once it's fired, but I'm having issues working with it wet sometimes. I have a feeling it might be the ratio for paper to clay that I've been using (I think I'm working with 30-40% paper). Anyone have any advice for me? Should I try another kind of fiber? ( For the paper, I just use single-ply toilet paper)

 

 

That seems like a high % of paper. My understanding is a maximum of 25%. Use anywhere from 15-25%

Marcia

 

 

 

I read in a book on paper clay that if you're wanting to sculpt with porcelain using paper clay then to use ~35% paper, but I'll try out a lesser % thank you

Share this post


Link to post
Share on other sites

Honestly, I just guess.

Porcelain paper clay is the only kind I mix myself, my stoneware is a commercially produced body that contains 10%-20% paper, depending on the body.

With the porcelain, I mix a slurry of toilet paper, water and bleach and then add it to the clay (which I've made into a slip).

No more than 20% paper, and its strong enough to withstand raku.

 

I've been using my own porcelain paper clay recipe for the past year or so. I love how it looks once it's fired, but I'm having issues working with it wet sometimes. I have a feeling it might be the ratio for paper to clay that I've been using (I think I'm working with 30-40% paper). Anyone have any advice for me? Should I try another kind of fiber? ( For the paper, I just use single-ply toilet paper)

 

 

That seems like a high % of paper. My understanding is a maximum of 25%. Use anywhere from 15-25%

Marcia

 

 

 

I read in a book on paper clay that if you're wanting to sculpt with porcelain using paper clay then to use ~35% paper, but I'll try out a lesser % thank you

 

Share this post


Link to post
Share on other sites

For patching I use a paste made in a blender with toilet paper or bits of paper from dried orange size paper that was made into pulp and strained. For working with paper clay I mix in a Soldner mixer and ad by dry volume.

 

Marcia

Share this post


Link to post
Share on other sites

Where do you find paper clay commercially? I have never used paper clay, because the process seems to intimidate me, but from what I've read I know I should. If I could buy it, all the better. Sandra

Honestly, I just guess.

Porcelain paper clay is the only kind I mix myself, my stoneware is a commercially produced body that contains 10%-20% paper, depending on the body.

With the porcelain, I mix a slurry of toilet paper, water and bleach and then add it to the clay (which I've made into a slip).

No more than 20% paper, and its strong enough to withstand raku.

 

I've been using my own porcelain paper clay recipe for the past year or so. I love how it looks once it's fired, but I'm having issues working with it wet sometimes. I have a feeling it might be the ratio for paper to clay that I've been using (I think I'm working with 30-40% paper). Anyone have any advice for me? Should I try another kind of fiber? ( For the paper, I just use single-ply toilet paper)

 

 

That seems like a high % of paper. My understanding is a maximum of 25%. Use anywhere from 15-25%

Marcia

 

 

 

I read in a book on paper clay that if you're wanting to sculpt with porcelain using paper clay then to use ~35% paper, but I'll try out a lesser % thank you

 

 

Share this post


Link to post
Share on other sites

For patching I use a paste made in a blender with toilet paper or bits of paper from dried orange size paper that was made into pulp and strained. For working with paper clay I mix in a Soldner mixer and ad by dry volume.

 

Marcia

 

 

 

Marcia, do you mean you strain the resulting slurry, the TP and clay combo, after it is blended? How fine are we talking about, I never thought of that. I will be up-grading my patching slip.

Share this post


Link to post
Share on other sites

Where do you find paper clay commercially? I have never used paper clay, because the process seems to intimidate me, but from what I

 

 

http://www.lagunacla...paper-clays.php

 

 

Thanks BigDave. I thought paper clay was great for sculpture for two reasons. First being as stated in the clay descriptions, is low shrinkage, but second an incredibly smooth texture for good fine details like you naturally get with porcelain. The grog confuses me. On this same note, what is B mix?

Thanks for your patience.

Sandradry.gif

Share this post


Link to post
Share on other sites

For patching I use a paste made in a blender with toilet paper or bits of paper from dried orange size paper that was made into pulp and strained. For working with paper clay I mix in a Soldner mixer and ad by dry volume.

 

Marcia

 

 

 

Marcia, do you mean you strain the resulting slurry, the TP and clay combo, after it is blended? How fine are we talking about, I never thought of that. I will be up-grading my patching slip.

 

 

In order to measure by volume, the paper slurry needs to be compressed. I strain it and get rid of the water and squeeze the remaining pulp into orange size lumps. Then, I can look at the dry volume and estimate 15%. For large quantities I am not using tp but paper linter.

Marcia

Share this post


Link to post
Share on other sites

 

 

Thanks BigDave. I thought paper clay was great for sculpture for two reasons. First being as stated in the clay descriptions, is low shrinkage, but second an incredibly smooth texture for good fine details like you naturally get with porcelain. The grog confuses me. On this same note, what is B mix?

Thanks for your patience.

Sandradry.gif

 

 

Yer Welcome...:rolleyes:src="http://ceramicartsdaily.org/community/public/style_emoticons/default/rolleyes.gif">

 

Id say you thought right..

.but after using mucho much of it

 

This Clay, doesn't attach incredibly well and isn't at all smooth..it is paper though...and commercial.... as requested...LOL

 

B-mix is the one right after A-mix...

 

I think

post-12771-136599277051_thumb.jpg

post-12771-136599277051_thumb.jpg

Share this post


Link to post
Share on other sites

I use 2 toilet rolls in a bucket of slip. Casted some really awesome and thin work with it. I was able to really break down the paper with my 'blender tool bit on the drill' and got a very smooth mix and a smooth slipcasted end-result.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.