Posted 20 March 2013 - 05:17 AM

I keep seeing the description "nuka glaze" on pieces I admire - a creamy white high fire glaze. Is nuka a kind of ash? I'd love to find a mid range recipe for this type of glaze but it probably doesn't exist...

#2 TJR

TJR

    Advanced Member

  • Members
  • PipPipPip
  • 1,821 posts
  • LocationWinnipeg,Manitoba,Canada

Posted 20 March 2013 - 09:27 AM

It's a soft, white-grey semi matt glaze. It does contain wood ash. I will post a recipe when I get to the studio.
John Baymore would be able to tell us more about it.
TJR.

#3 JBaymore

JBaymore

    Moderator

  • Moderators
  • 4,125 posts
  • LocationWilton, NH USA

Posted 20 March 2013 - 10:50 PM

Writing from NCECA.....working totally from memory here.... my glaze file is not here.

"Nuka" is the Japanese word for the husk (or hull) of the rice kernel. It is a by-product of the milling of white rice. The Japanese version is from a short grain rice.

Potter parlance (in Japanese) uses this term for glazes based upon rice HUSK ash (not rice straw ash....... different chemical composition). The agricultural waste is piled in the fields and is then burned. The piles smolder more than burn, and a good ash for glaze use is actually dark grey to black. You don't want it to burn cleanly. This color comes from carbon residue in the ash. SO the ash has a high L.O.I. The chemical composition of rice husk ash (after L.O.I.) is almost colloidally fine silica. (TJR I'd call it more of a semi-gloss.)

Nuka glazes are high calcium fluxed glazes (from the washed wood ash) what use the rice husk ash for a lot of the silica content, and bringing in the silica in a very fine particle size. They fire a bluish white and are slightly milky opaque where thicker due to the unmelted silica particles.

I use real rice husk ash (imported and expensive) and washed hardwood ash. Firing it from Orton cone 10 to Orton cone 14. The recipe I started with I got from Hamada Shoji-sensei.

1/3 rice husk ash
1/3 wood ash
1/3 terayama stone ( a high silica bearing feldspathoid)


That is modified for more locally available materials as...............


32% rice husk ash

32% wood ash

32% Custer feldspar

4% flint

This stuff is natural material glaze.... the slurry handles VERY differently from what most people are used to when ucing commercial beneficiated materials. It looks REALLY thick when on the proper consistency, and is sort of "fuzzy" looking. It setles down in firing due to the high L.O.I. of the rice husk ash.

Hope this is of use.


best,

...................john

John Baymore
Professor of Ceramics; New Hampshire Insitute of Art

Guest Professor, Wuxi Institute of Arts and Science, Yixing, China

Former President and Past President; Potters Council
 

http://www.JohnBaymore.com

http://www.nhia.edu/...ty/john-baymore


#4 Natania

Natania

    Advanced Member

  • Members
  • PipPipPip
  • 200 posts
  • LocationMassachusetts

Posted 21 March 2013 - 05:15 AM

Writing from NCECA.....working totally from memory here.... my glaze file is not here.

"Nuka" is the Japanese word for the husk (or hull) of the rice kernel. It is a by-product of the milling of white rice. The Japanese version is from a short grain rice.

Potter parlance (in Japanese) uses this term for glazes based upon rice HUSK ash (not rice straw ash....... different chemical composition). The agricultural waste is piled in the fields and is then burned. The piles smolder more than burn, and a good ash for glaze use is actually dark grey to black. You don't want it to burn cleanly. This color comes from carbon residue in the ash. SO the ash has a high L.O.I. The chemical composition of rice husk ash (after L.O.I.) is almost colloidally fine silica. (TJR I'd call it more of a semi-gloss.)

Nuka glazes are high calcium fluxed glazes (from the washed wood ash) what use the rice husk ash for a lot of the silica content, and bringing in the silica in a very fine particle size. They fire a bluish white and are slightly milky opaque where thicker due to the unmelted silica particles.

I use real rice husk ash (imported and expensive) and washed hardwood ash. Firing it from Orton cone 10 to Orton cone 14. The recipe I started with I got from Hamada Shoji-sensei.

1/3 rice husk ash
1/3 wood ash
1/3 terayama stone ( a high silica bearing feldspathoid)


That is modified for more locally available materials as...............


32% rice husk ash

32% wood ash

32% Custer feldspar

4% flint

This stuff is natural material glaze.... the slurry handles VERY differently from what most people are used to when ucing commercial beneficiated materials. It looks REALLY thick when on the proper consistency, and is sort of "fuzzy" looking. It setles down in firing due to the high L.O.I. of the rice husk ash.

Hope this is of use.


best,

...................john




Thank you very much. Extremely informative. What is L.O.I.?

#5 JBaymore

JBaymore

    Moderator

  • Moderators
  • 4,125 posts
  • LocationWilton, NH USA

Posted 21 March 2013 - 08:23 AM

Loss On Ignition. It is the difference in molecular weight when the material has been heated up to reactive temperature / oxidized in the kiln and the starting molecular weight In this case carbonaceous matter gets turned to CO2 and things like carbonates give up the CO2.

best,

....................john

John Baymore
Professor of Ceramics; New Hampshire Insitute of Art

Guest Professor, Wuxi Institute of Arts and Science, Yixing, China

Former President and Past President; Potters Council
 

http://www.JohnBaymore.com

http://www.nhia.edu/...ty/john-baymore


#6 phill

phill

    Advanced Member

  • Members
  • PipPipPip
  • 222 posts
  • Locationmn

Posted 24 October 2014 - 09:22 PM

Hey John, where or from what website do you purchase your rice husk ash? Do you always have to buy in massive bulk containers?



#7 Wyndham

Wyndham

    Advanced Member

  • Members
  • PipPipPip
  • 486 posts
  • LocationSeagrove NC

Posted 25 October 2014 - 07:50 AM

saw something the other day about rice husk being a waste product from milling in California rice production. I had have to google to find it but will look into it later.It's being re purposed into something, forget what???

 BTY John what about Michael Coffee's Nuka

  • Custer Feldspar    36.00
  • Quartz   30.00
  • Whiting   22.00
  • OM-4   6.00
  • Wood Ash (unwashed)   3.00
  • Talc   2.00
  • Bone Ash   2.00

http://dmichaelcoffe...-∆10-reduction/

 

Notes: This a ∆10 Reduction glaze that will fire to a Creamy White with low gloss to satiny finish. Good over tenmoku, will run if applied too thick over thick tenmoku. As always, test for your ingredient and firing conditions.

 

I use on version that breaks white/green on top of a rutile blue

 

have to look for it later

 

Wyndham



#8 phill

phill

    Advanced Member

  • Members
  • PipPipPip
  • 222 posts
  • Locationmn

Posted 25 October 2014 - 08:18 AM

Thanks Wyndham for the recipe. I have seen this before but I completely forgot about it! I like that this glaze is not shiny white but rather satin white. Now I would just need to find wood ash. No one here in MN seems to have any for me, and I don't have a fire pit. 



#9 Wyndham

Wyndham

    Advanced Member

  • Members
  • PipPipPip
  • 486 posts
  • LocationSeagrove NC

Posted 25 October 2014 - 09:26 AM

Phil, look up the equivalent of wood ash in chemicals we use.3% will not be much more than a few flux ingrediends

Wyndham



#10 Wyndham

Wyndham

    Advanced Member

  • Members
  • PipPipPip
  • 486 posts
  • LocationSeagrove NC

Posted 25 October 2014 - 12:55 PM

John, Here's the link I was looking for

\

http://www.environme...nt-tire-treads/

 

I bet they might share some for a pot to go in the boardroom

Wyndham



#11 JBaymore

JBaymore

    Moderator

  • Moderators
  • 4,125 posts
  • LocationWilton, NH USA

Posted 25 October 2014 - 02:12 PM

Wyndham,

 

That glaze recipe above is what you might call a 'synthetic nuka'.  Similar look.  I believe that a number of potters have their name on variations of that kind of glaze.

 

I've been in contact with a US supplier of by-product rice husk ash from electric generation.  Unfortunately to work well for a glaze, it reallty has to be burned in a certain way.  That stuff is not.  Would likely require a lot of "processing" on the user's end to get it suitable.

 

best,

 

..............john


John Baymore
Professor of Ceramics; New Hampshire Insitute of Art

Guest Professor, Wuxi Institute of Arts and Science, Yixing, China

Former President and Past President; Potters Council
 

http://www.JohnBaymore.com

http://www.nhia.edu/...ty/john-baymore


#12 phill

phill

    Advanced Member

  • Members
  • PipPipPip
  • 222 posts
  • Locationmn

Posted 26 October 2014 - 10:01 AM

ahh okay interesting.

 

John, do you buy unburned rice husk then? How do you get your supply?



#13 JBaymore

JBaymore

    Moderator

  • Moderators
  • 4,125 posts
  • LocationWilton, NH USA

Posted 26 October 2014 - 10:56 AM

Phil,

 

As mentioned way above..... I import it.  And it is the most expensive glaze ingredient I buy because of that.  But the real thing and the synthetic recipes do look different if you are looking closely.  I reserve it almost 100% for Chawan.

 

It is the burnerd ash... not the husks.  The husks burn down a huge amount (probably 80 percent)..... so while light... they are voluminous and would be crazy to ship.

 

best,

 

..................john


John Baymore
Professor of Ceramics; New Hampshire Insitute of Art

Guest Professor, Wuxi Institute of Arts and Science, Yixing, China

Former President and Past President; Potters Council
 

http://www.JohnBaymore.com

http://www.nhia.edu/...ty/john-baymore


#14 jrgpots

jrgpots

    The hands can express the soul

  • Members
  • PipPipPip
  • 764 posts
  • LocationHurricane, Utah

Posted 09 November 2014 - 04:23 PM

Wyndham,


I've been in contact with a US supplier of by-product rice husk ash from electric generation. Unfortunately to work well for a glaze, it reallty has to be burned in a certain way. That stuff is not. Would likely require a lot of "processing" on the user's end to get it suitable.

best,

..............john


This may be a silly question....But... do you know what is the special way to burn the husks? I'd like to refine my tumbleweed ash a bit to improve my ash glaze.

Jed

#15 JBaymore

JBaymore

    Moderator

  • Moderators
  • 4,125 posts
  • LocationWilton, NH USA

Posted 09 November 2014 - 08:47 PM

Jed,

 

Because the husks in a pile are so dense... unlike your relatively open tumbleweeds....... getting air into the pile is the issue for burning.  Usually a sort of a metal chimney is imbeded into the pile and moved around.  The piles 'smoulder' rather than a real "burn" really.  For the glazes... it needs to be burned so that it is partially burned.... and is pretty much black or dark grey.  Huge LOI when the glaze is fired.

 

best,

 

.................john


John Baymore
Professor of Ceramics; New Hampshire Insitute of Art

Guest Professor, Wuxi Institute of Arts and Science, Yixing, China

Former President and Past President; Potters Council
 

http://www.JohnBaymore.com

http://www.nhia.edu/...ty/john-baymore


#16 phill

phill

    Advanced Member

  • Members
  • PipPipPip
  • 222 posts
  • Locationmn

Posted 22 November 2014 - 08:06 PM

This may be a silly question....But... do you know what is the special way to burn the husks? I'd like to refine my tumbleweed ash a bit to improve my ash glaze.

Jed


Check out this chimney firing for burning brush. Seems like a great idea!






1 user(s) are reading this topic

0 members, 1 guests, 0 anonymous users