Just an observation here. I throw plates/patens for communion services. The group that I throw them for requires a rubber stamped logo on the plate surface. When trimming these, I notice that I always have a difficult time staying even across the foot indent. I have finally realized that it isn't me, it is the stamped area with higher compression that makes it difficult to get an even cut. This occurs whether I stamp into the wet clay, or the cheese hard clay. I use loop tools to trim, and keep them sharp. I also use a flat metal rib held perpendicular across the center lately and that seems to do the best job. Any suggestion?

Share this post


Link to post
Share on other sites
AtomicAxe    19

It could just be the compression and displacement of clay AROUND the stamp ... have you tried using a rib to heavily compress your plate surface before stamping?

Share this post


Link to post
Share on other sites
Pres    896

It could just be the compression and displacement of clay AROUND the stamp ... have you tried using a rib to heavily compress your plate surface before stamping?

 

 

I always compress the plates heavily with a wooden rib in the beginning, and then with a rubber rib for smoother surface. I am certain it is because of the compression around the stamped area long with displacement. The only thing that seems to even it out is the large straight hack saw blade over the center once trimmed down. I don't place the stamp in the center more at 10, 2, 4 or 8 on the clock half way from center to edge.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×