Posted 06 March 2013 - 11:25 PM

I have thrown for a few years now and i am used to clay that has little grit and is around cone 4-6. Could someone recommend types of clay that would suit my needs?
Practice, practice, practice. Then when you think you've practiced enough, the real practice begins.

#2 GEP

GEP

    Moderator / full time potter ^6 stoneware

  • Moderators
  • 1,354 posts
  • LocationSilver Spring, MD

Posted 07 March 2013 - 12:17 AM

Do you have a particular color in mind?

Mea
Mea Rhee
Good Elephant Pottery
http://www.goodelephant.com

#3 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,144 posts
  • LocationRed Lodge, Montana

Posted 07 March 2013 - 07:43 AM

It would help to mention your location because suppliers array some same clays like Laguna and others carry their own like Armadillo.
XThat is a big geographical spread. Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#4 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 4,828 posts
  • LocationGrayslake, IL

Posted 07 March 2013 - 09:17 AM

The closest suppliers to Cambridge, WI are A.R.T. in Sturtevant, or Paoli Clay, or Ceramic Supply Chicago in Evanston, IL or Great Lakes Clay in Elgin, IL. I'm not a big fan of any of then except Ceramic Supply Chicago. I buy about 25,000 pounds from them every year. What color clay are you looking for, brown or white?

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

[email protected]


#5 Rebekah Krieger

Rebekah Krieger

    The extraordinary clay bender

  • Members
  • PipPipPip
  • 786 posts
  • LocationWisconsin

Posted 07 March 2013 - 10:06 AM

I live in se wisconsin and i drive to ART so save on shipping, the problem is that every time I order on the phone they get my order wrong. I just got the 3rd wrong order within 3 months from them yesterday

~ Namaste ~

 

Home studio potter 

 

Shanel Pottery 

www.shanelpottery.com

www.facebook.com/shanelspottery 

 

 

 

"To me the greatest thing is to live beauty in our daily life and to crowd every moment with things of beauty.  It is then, and then only that  the art of the people as a whole is endowed with it's richest significance.  For it's products are those made by great a many craftsmen for the mass of the people, and the moment this art declines the life of the nation  is removed far away from beauty.  So long as beauty abides in only in a few articles created by a few geniuses, the kingdom of beauty is nowhere near realization."                                                                                 - Bernard Leach 

#6 bciskepottery

bciskepottery

    Advanced Member

  • Moderators
  • 2,672 posts
  • LocationNorthern Virginia

Posted 07 March 2013 - 11:47 AM

The closest suppliers to Cambridge, WI are A.R.T. in Sturtevant, or Paoli Clay, or Ceramic Supply Chicago in Evanston, IL or Great Lakes Clay in Elgin, IL. I'm not a big fan of any of then except Ceramic Supply Chicago. I buy about 25,000 pounds from them every year. What color clay are you looking for, brown or white?



I believe you can order clay from/through NASCO in Fort Atkinson -- just a short drive from Cambridge.

http://www.enasco.co...t clay&x=20&y=8

#7 Davidpotter

Davidpotter

    Determined Young Buck

  • Members
  • PipPipPip
  • 70 posts
  • LocationNeenah, Wisconsin

Posted 07 March 2013 - 07:47 PM

i would like brown clay and yes I live in Cambridge and i don't really want to drive to IL. thank you for the replys.
Practice, practice, practice. Then when you think you've practiced enough, the real practice begins.

#8 GEP

GEP

    Moderator / full time potter ^6 stoneware

  • Moderators
  • 1,354 posts
  • LocationSilver Spring, MD

Posted 08 March 2013 - 09:50 AM

I have been trying out different cone 6 brown clays lately, I like:

Standard 112, medium brown with heavy speckles
Standard 266, very dark espresso brown
Highwater Brownstone, very similar to Standard 112, but can be had with or without speckles
Highwater Red Rock, reddish brown with speckles

Even if your local supplier does not have these specific clays, they probably buy clay from Standard and Highwater, and could probably order them for you.

Good luck!

Mea
Mea Rhee
Good Elephant Pottery
http://www.goodelephant.com

#9 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 4,828 posts
  • LocationGrayslake, IL

Posted 08 March 2013 - 10:24 AM

Standard 112 is one of my all time favorite stoneware clays. Excellent stuff! They also have a non-speckled version. Ceramic Supply Chicago in Evanston carries Standard clays. IMO they are the best clays in the area by far. You could always make a day of it and spend the day in the city. When I lived in Iowa I used to drive 4 hours up to Minneapolis to get clay and we'd spend the day seeing the city.

Or I can get it in to my shop for you. I'll be placing an order in the next week. Im only about 1:40 from Cambridge. Just take Hwy 12 to Volo then take Hwy 120 about 10 miles east. I drive it each day for the pottery festival. It's a nice drive.

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

[email protected]





0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users