Hi... I am interested in firing to cone 6 with my Skutt KM 1018. I am playing with stoneware and porcelain. What cone do I use to bisque? Also,which speed do I use for bisque and final firing (slow, med or fast)? I am in no rush... Last question--should I use "ramp/hold"? I've been reading about holding at certain temps for specific amounts of time, but I truly have no idea where to start. I've fired to cone 04 for years and need a change. I would LOVE any help, my greenware is piling up. Thanks in advance!

#2 Mark McCombs

Mark McCombs

    Advanced Member

  • Members
  • PipPipPip
  • 123 posts
  • LocationSW Washington

Posted 27 February 2013 - 11:53 AM

Hi Marge,

I would bisque to cone 04 at a medium rate. I only use the ramp/hold feature when the ware is somewhat think or I suspect it might not be bone dry.
With the ramp hold, I can add a segment for candling to make sure the ware is dry before continuing with the firing.

Use a medium fire rate for the glaze (^6) fire too.

I also use ramp/hold for controlled cooling on glaze fires.

Contact Skutt and they can send you a spreadsheet showing the segments for all the cone to use with the ramp/feature.


Posted Image
Mark
Fast Hawk Pottery


^5-6 Ox
1227 Skutt

#3 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 4,828 posts
  • LocationGrayslake, IL

Posted 27 February 2013 - 01:34 PM

Medium speed will work fine for most anything. If you have large or thick pots you may want to bisque on slow.

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

[email protected]


#4 Marge

Marge

    Member

  • Members
  • PipPip
  • 25 posts

Posted 27 February 2013 - 02:10 PM

Thanks so much!! I can't wait to startPosted Image

#5 Jo-Ann

Jo-Ann

    Advanced Member

  • Members
  • PipPipPip
  • 60 posts
  • LocationOntario, Canada

Posted 27 February 2013 - 07:48 PM

Hi, I have a skutt but someone a while ago gave me a firing poster for paragon. . . It helped a lot with getting me comfortable with my kiln and giving me a place to start . . . Maybe it can help you . . .

http://www.paragonwe...s/A-82B-FSP.pdf

I have also used this poster

http://www.stonemoun...iring_Chart.pdf

#6 Denice

Denice

    Advanced Member

  • Members
  • PipPipPip
  • 1,217 posts
  • LocationWichita, Kansas

Posted 28 February 2013 - 09:42 AM

The paragon chart is the same one that was with my paragon kiln that I bought over 40 years ago and still fire, the other chart looks like it would be easy for a novice to use. Denice




0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users