I am wondering if it is possible to successfully apply maiolica on bone dry pots and fire once to cone 04. I am wanting to skip the bisque firing if possible. I have a computerized kiln so I can program a slow firing cycle with a controlled cooling cycle. Any suggestions would be appreciated.

Share this post


Link to post
Share on other sites

Lee Love said he does this recently on clay art.

However, firing majolica after a bisque was the whole reason bisque firing started.

Majolica was invented to impersonate proto-porcelain in the Persian empire about 9th-10 century after a huge battle

with the Chinese..late Tang Dynasty. The Persians had only a gritty low fire clay sometimes iron bearing. The court chemists developed the opaque white glaze

to cover the non-white clay. Bisque firing was introduced to keep the impurities of the raw clay body from contaminating the white glaze.

Today potters use bisque firing much more frequently than in the past.

-Marcia

Share this post


Link to post
Share on other sites

Lee Love said he does this recently on clay art.

However, firing majolica after a bisque was the whole reason bisque firing started.

Majolica was invented to impersonate proto-porcelain in the Persian empire about 9th-10 century after a huge battle

with the Chinese..late Tang Dynasty. The Persians had only a gritty low fire clay sometimes iron bearing. The court chemists developed the opaque white glaze

to cover the non-white clay. Bisque firing was introduced to keep the impurities of the raw clay body from contaminating the white glaze.

Today potters use bisque firing much more frequently than in the past.

-Marcia

 

 

PS if you try raw glazing, add 5% bentonite to the glaze.

Marcia

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.