Posted 24 February 2013 - 09:28 PM

For fun I got a small jar of 2004 high temperature black stain. No where on the jar does it give mixing instructions. I use white stoneware clay and have a lot of dried trimmings but have no clue where to start with stain to dry clay ratio. I sent an email to spectrum last week; no reply yet. I'll experiment but a starting point would be helpful. Thanks :)

#2 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,116 posts
  • LocationRed Lodge, Montana

Posted 25 February 2013 - 12:19 PM

Some underglaze recipes use as much as 25% stain. If the black is strong, start with 10% and add a few grams. Fire the tests and see what increments work best for you.

Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#3 Jo-Ann

Jo-Ann

    Advanced Member

  • Members
  • PipPipPip
  • 60 posts
  • LocationOntario, Canada

Posted 25 February 2013 - 12:43 PM

Start at 10%. Thank you so much!!!!