I've just returned from teaching a colored clay workshop using Skinner Blends at the John C Campbell Folk School ... very fun!!!
Mike Lalonde, the resident potter, volunteered to throw some Skinner slabs for me since my throwing skills are rusty. We folded the slabs, drop wedged so the colors would not get mixed ... he threw the slabs in all the ways we could think of and got some wonderful results. I carved on the cups to see what would happen.

So, YES ... finally I know that Skinner blended colored clays can be thrown with great results.
I am so thrilled with it that I might just have to start throwing again!
Here are a couple images, but more to follow once I get better shots.

Attached Files


Chris Campbell Pottery
Contemporary Fine Colored Porcelain
http://ccpottery.com/

>TRY ... FAIL ... LEARN ... REPEAT"

" If a sufficient number of people are different, no one has to be normal "

Fredrick Bachman

#2 docweathers

docweathers

    Gismo Guy

  • Members
  • PipPipPip
  • 643 posts
  • LocationSpokane Wa

Posted 18 February 2013 - 12:15 AM

and Skinners slabs are??

Larry

Lawrence Weathers

Gismo Guy

Spokane WA


#3 Mark C.

Mark C.

    Advanced Member

  • Members
  • PipPipPip
  • 6,310 posts
  • LocationNear Arcata Ca-redwood rain forest

Posted 18 February 2013 - 04:00 AM

I'm not from the south but are they not skinned squirrels of various colors then blended in a blender and rendered down to basic goo and added to white clays with when the fur burns off causes color streaks in clay??
I may have this confused with squirrel stew process its where you drink the warm stew after burning the hair off some slow moving squirrels.The smell reminds you of why you should have skinnered them first.
It also may be a blended bar drink called a skinner blend or shot- one part bourbon two parts gun oil-then after 4 drinks you can catch and skin a squirrel and get your skinner badge.
The south has some strange customs like pepmo pink interiors for hanging squirrel skins and shooting down a few skinner shots.
I have also heard of potters who have guns in the studio to blast visitors who come looking for them facing the wall.And if its a slow day they shoot pots.
The south I suggest giving it a WIDE berth.
Mark

PS this whole post is in jest.
Mark Cortright
www.liscomhillpottery.com

#4 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,348 posts
  • LocationRed Lodge, Montana

Posted 18 February 2013 - 08:12 AM

Chris,
Looks like you gave a very successful workshop that went in all directions.
Congrats!

Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#5 OffCenter

OffCenter

    Advanced Member

  • Members
  • PipPipPip
  • 1,372 posts

Posted 18 February 2013 - 09:33 AM

I'm not from the south but are they not skinned squirrels of various colors then blended in a blender and rendered down to basic goo and added to white clays with when the fur burns off causes color streaks in clay??
I may have this confused with squirrel stew process its where you drink the warm stew after burning the hair off some slow moving squirrels.The smell reminds you of why you should have skinnered them first.
It also may be a blended bar drink called a skinner blend or shot- one part bourbon two parts gun oil-then after 4 drinks you can catch and skin a squirrel and get your skinner badge.
The south has some strange customs like pepmo pink interiors for hanging squirrel skins and shooting down a few skinner shots.
I have also heard of potters who have guns in the studio to blast visitors who come looking for them facing the wall.And if its a slow day they shoot pots.
The south I suggest giving it a WIDE berth.
Mark


That's funny, Mark. I enjoyed it. If you're ever down this way I'll buy you a skinner blend.

Jim
E pur si muove.

"But it does move," said Galileo under his breath.

#6 DallasGypsy

DallasGypsy

    Advanced Member

  • Members
  • PipPipPip
  • 33 posts
  • LocationFlorida

Posted 18 February 2013 - 10:23 AM

What are Skinner blends & Skinner slabs?

#7 bciskepottery

bciskepottery

    Advanced Member

  • Moderators
  • 2,703 posts
  • LocationNorthern Virginia

Posted 18 February 2013 - 11:55 AM


I'm not from the south but are they not skinned squirrels of various colors then blended in a blender and rendered down to basic goo and added to white clays with when the fur burns off causes color streaks in clay??
I may have this confused with squirrel stew process its where you drink the warm stew after burning the hair off some slow moving squirrels.The smell reminds you of why you should have skinnered them first.
It also may be a blended bar drink called a skinner blend or shot- one part bourbon two parts gun oil-then after 4 drinks you can catch and skin a squirrel and get your skinner badge.
The south has some strange customs like pepmo pink interiors for hanging squirrel skins and shooting down a few skinner shots.
I have also heard of potters who have guns in the studio to blast visitors who come looking for them facing the wall.And if its a slow day they shoot pots.
The south I suggest giving it a WIDE berth.
Mark


That's funny, Mark. I enjoyed it. If you're ever down this way I'll buy you a skinner blend.

Jim


Mark C -- I belive you might be thinking of Skinner's pigeons; he is far more famous for his work with pigeons than squirrels. He tried squirrels, but the pesky little varmints attention spans were too short.

#8 bciskepottery

bciskepottery

    Advanced Member

  • Moderators
  • 2,703 posts
  • LocationNorthern Virginia

Posted 18 February 2013 - 11:56 AM

What are Skinner blends & Skinner slabs?



http://ceramicartsda...ng-illustrated/

#9 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,116 posts
  • LocationRaleigh, NC

Posted 18 February 2013 - 12:22 PM

SORRY !!!! I am so into it that I think everybody knows what I'm talking about.
Yes ... reference PMI January 2013

Skinner Blend slabs are slabs of clay color blends created with a slab roller ... I had only used them for hand building so it was great to see thrown results.
We sliced them in all directions, slam wedged them so the colors would not blend, then threw them with only one or two pulls.
I'll be teaching again in April so might have more examples then.

Attached Files


Chris Campbell Pottery
Contemporary Fine Colored Porcelain
http://ccpottery.com/

>TRY ... FAIL ... LEARN ... REPEAT"

" If a sufficient number of people are different, no one has to be normal "

Fredrick Bachman

#10 OffCenter

OffCenter

    Advanced Member

  • Members
  • PipPipPip
  • 1,372 posts

Posted 18 February 2013 - 01:42 PM

SORRY !!!! I am so into it that I think everybody knows what I'm talking about.
Yes ... reference PMI January 2013

Skinner Blend slabs are slabs of clay color blends created with a slab roller ... I had only used them for hand building so it was great to see thrown results.
We sliced them in all directions, slam wedged them so the colors would not blend, then threw them with only one or two pulls.
I'll be teaching again in April so might have more examples then.


Great job, Chris. Now, if you can just get porcelain to work as reducible canes.

Jim
E pur si muove.

"But it does move," said Galileo under his breath.

#11 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,116 posts
  • LocationRaleigh, NC

Posted 18 February 2013 - 04:02 PM

"Great job, Chris. Now, if you can just get porcelain to work as reducible canes. "

Yeah ... I would enjoy that a lot too!! I have tried and tried again with little success.
Chris Campbell Pottery
Contemporary Fine Colored Porcelain
http://ccpottery.com/

>TRY ... FAIL ... LEARN ... REPEAT"

" If a sufficient number of people are different, no one has to be normal "

Fredrick Bachman




0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users