Inherited glaze materials

Recommended Posts

mayaearth    0

I've recently been given access to a studio full of glaze materials! Is there any concern that certain materials could go bad, or stale, as they've been sitting for several years? Everything has been stored in lidded jars and buckets. Also, a few of the jars have lost their labels. Is there any way to go about identifying the mystery materials?

Share this post


Link to post
Share on other sites
JBaymore    1,432

I've recently been given access to a studio full of glaze materials! Is there any concern that certain materials could go bad, or stale, as they've been sitting for several years? Everything has been stored in lidded jars and buckets. Also, a few of the jars have lost their labels. Is there any way to go about identifying the mystery materials?

 

 

Remember that such an "find" may end up being a liability in the end.

 

The un-labeled buskets are particulary problematic. Technically they are "hazardous waste", since you have no idea what is in them. A white powder could be EPK... or white lead....or lithium carbonate... or barium carbonate.... or even something not at all related to ceramics like pool chlorine .... or fertilizer..... or ?????????. If you have to dispose of them yourself, it will likely cost you..... particulary if you sell your work (are thereby a "business").

 

Identifying such stuff is certainly possible.... a lab can test them .... but it will not be inexpensive. Glaze materials are cheap.... not going to be worth that expense.

 

Otherwise.... no, the materials generally do not "go bad". Stuff like organic gums can cake up due to atmospheric moisture... and be such a pain to use that they are worthless. But stuff like feldspars and flint and such generally are OK if they are not seriously wetted. And then if they do get wet....... they'll just clump up and you'll need to seive more carefully after you dry them out and are using them. Clays, if they get wet, will be a bit more problematic..... but possibly could still be used.

 

If they are really old materials... the materials analysis may not match current materials sources. So some glaze recipes may look a tad different.

 

best,

 

.....................john

Share this post


Link to post
Share on other sites
Mark C.    1,798

As John said the mystery materials are to expensive to figure out-I would toss them-Label everything NOW so the rest of the labels are permanent and can not fall off.

If these are from a yesteryear you may have some things that are not around much anymore like carbonated lead or white lead both are nasty.

 

Most materials keep forever. One last note if you know a working potter they may be able to discern one or two of those unidentified materials as a few have certain unique qualities .

Keep them dry.

Mark

Share this post


Link to post
Share on other sites
Mark C.    1,798

As John said the mystery materials are to expensive to figure out-I would toss them-Label everything NOW so the rest of the labels are permanent and can not fall off.

If these are from a yesteryear you may have some things that are not around much anymore like carbonated lead or white lead both are nasty.

Most materials keep forever.

One last note if you know a working potter they may be able to discern one or two of those unidentified materials as a few have certain unique qualities Keep them dry.

Mark

Share this post


Link to post
Share on other sites
Marcia Selsor    1,301

You can not just toss potentially hazardous chemicals. It could get you in trouble, like a big fine from the EPA if you get caught. You could donate it to a local college and maybe they could figure out what they are.

They would also have the means of disposing hazardous chemicals.

 

 

Marcia

Share this post


Link to post
Share on other sites
mayaearth    0

The unidentified materials are minimal, a few pounds at most. It's good to know that the materials are still good and, of course, I'm starting with test batches.Thanks so much for the response!

Share this post


Link to post
Share on other sites
Mark C.    1,798

The unidentified materials are minimal, a few pounds at most. It's good to know that the materials are still good and, of course, I'm starting with test batches.Thanks so much for the response!

 

 

We have a hazard waste drop off twice a year for 5$ they take it in hazmat suits-This service travels around our county.This is what I have done in the past-I did not mean just toss it in trash.You can call your local dump on when this drop off is scheduled.

Mark

Share this post


Link to post
Share on other sites
Marcia Selsor    1,301

That is a nice service to have. When I was teaching, the haz-mat office of the campus did regular inspections and provided containers for

hazardous materials.

 

Marcia

Share this post


Link to post
Share on other sites
JBaymore    1,432
We have a hazard waste drop off twice a year for 5$ they take it in hazmat suits-This service travels around our county.This is what I have done in the past-I did not mean just toss it in trash.You can call your local dump on when this drop off is scheduled.

 

Wow ... the only kinds of this thing around here are "Household" hazardous waste pickup days twice a year. If you are a business... they won't take the stuff and in fact seriptitiously using it (if you are a buusiness) is illegal.

 

OK for hobby potters though.

 

best,

 

.....................john

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×