glaze after 1200 fire

Recommended Posts

1200 C would be about ^5. You may have vitrified the clay body depending on the type of clay you are using.

Some glazes may still cling to the surface. You can try heating the pots before trying to glaze. You can try adding a little gum to the glaze and spray it on..

 

Marcia